hottub.patents
Assignee / Organization

Okinaka Hideyuki

40Total Forward Citations
7Indexed Patents
6Avg Citations / Patent
4Portfolio H-Index
WO 02,090,117 A1#6211241 Most Cited · 15 citations0.6/yr · PR 3.14PendingWO · Application
Ink jet device, ink jet ink, and method of manufacturing electronic component using the device and the ink

An ink jet device having an ink circulation function and an ink distribution function, wherein the ink used is re-distributed as necessary, and a part of the ink is fed to a printer head while the ink is fed to an ink colleting tank through a tube to form a specified pattern on…

WO 9,938,176 A1#8912411 Most Cited · 11 citations0.4/yr · PR 3.33PendingWO · Application
Ink for electronic component, method for producing electronic component by using the ink for electronic component, and ink-jet device

The invention relates to an ink for electronic components used for multilayer ceramic capacitors, LC filters, and composite high-frequency components, a method for producing an electronic component using the ink, and an ink-jet device. An ink for electronic components which…

WO 2012/046765 A1#13646727 Most Cited · 8 citations0.6/yr · PR 1.69PendingWO · Application
Non-linear resistive element and manufacturing method thereof

The disclosed manufacturing method of non-linear resistive elements ensures compositional and microstructural uniformity of the ceramic sintered body while enlarging the surface area of the ceramic sintered body, and leads to improved basic performance consisting of…

US 8,896,409 B2#26899312 Most Cited · 4 citations0.3/yr · PR 1.14ActiveUS · Utility
Non-linear resistive element and manufacturing method thereof
Inventors: Okinaka Hideyuki, Tsukamoto Naoyuki, Suzuki Toshihiko, Otsuki HiroyukiAssignee: Okinaka Hideyuki, Tsukamoto NaoyukiFiled 2011-10-05 · Granted 2014-11-25

Provided is a technique to secure compositional or microstructural uniformity of a ceramic sintered body while increasing the area of the ceramic sintered boy, thus improving basic performance including non-linearity, maximum withstand energy and aging characteristics. A…

US 2013169405 A1#44251612 Most Cited · 2 citations0.1/yr · PR 0.91PendingUS · Application
Non-linear resistive element and manufacturing method thereof

Provided is a technique to secure compositional or microstructural uniformity of a ceramic sintered body while increasing the area of the ceramic sintered boy, thus improving basic performance including non-linearity, maximum withstand energy and aging characteristics. A…

WO 02,090,117 B1#91214800 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Ink jet device, ink jet ink, and method of manufacturing electronic component using the device and the ink

An ink jet device having an ink circulation function and an ink distribution function, wherein the ink used is re-distributed as necessary, and a part of the ink is fed to a printer head while the ink is fed to an ink colleting tank through a tube to form a specified pattern on…

WO 9,900,808 A1#86078788 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Electronic part and method for producing the same

A method for producing an electronic part employed in a multilayer ceramic part, in which the conventional step of grinding the multilayer sintered block for the connection of the inner electrodes of the electronic part to the outer electrodes is omitted and by which the…