A steel for steel pipes which comprises, on the percent by mass basis, C: 0.2 to 0.7%, Si: 0.01 to 0.8%, Mn: 0.1 to 1.5%, S: 0.005% or less, P: 0.03% or less, Al: 0.0005 to 0.1%, Ti: 0.005 to 0.05%, Ca: 0.0004 to 0.005%, N: 0.007% or less, Cr: 0.1 to 1.5%, Mo: 0.2 to 1.0%, Nb: 0…
Numata Mitsuhiro
Disclosed is steel for a steel pipe, which satisfies a plurality of characteristics at the same time. Specifically disclosed is steel for a steel pipe having excellent sulfide stress cracking resistance, which contains, in mass%, 0.2-0.7% of C, 0.01-0.8% of Si, 0.1-1.5% of Mn,…
A steel product for a line pipe, which has a chemical composition, in mass %, that C: 0.03 to 0.15 %, Si: 0.05 to 1.0 %, Mn; 0.5 to 1.8 %, P: 0.015 % or less, S: 0.004 % or less, O: 0.01 % or less, N: 0.007 % or less, Sol.Al: 0.01 to 0.1 %, Ti: 0.024 % or less, Ca: 0.0003 to…
The steel for steel pipes of the present invention is the one for steel pipes excellent in sour-resistance performance including C, Mn, Si, P, S, Ti, Al, Ca, N and O, and optionally including a predetermined amount of one or more of Cr, Ni, Cu, Mo, V, B and Nb, in which…
The present invention provides a steel which simultaneously satisfies a plurality of characteristics, specifically, a steel for tubes with excellent sulfide stress cracking resistance, including, C: 0.2 to 0.7%; Si: 0.01 to 0.8%; Mn: 0.1 to 1.5%; S: not more than 0.005%; P: not…
Provided is a steel oil well pipe which has excellent sulfide stress cracking resistance (SSC resistance). A steel oil well pipe of the present invention contains, in mass%, 0.15-0.35% of C, 0.1-0.75% of Si, 0.1-1.0% of Mn, 0.1-1.7% of Cr, 0.1-1.2% of Mo, 0.01-0.05% of Ti,…
A method of producing steel for a steel pipe excellent in sour-resistance performance comprises controlling the amount of Ca addition charged into a molten steel in a ladle according to a N content in the molten steel prior to Ca addition. Non-metallic inclusions in the steel…
The present invention provides a steel which simultaneously satisfies a plurality of characteristics, specifically, a steel for tubes with excellent sulfide stress cracking resistance, including, C: 0.2 to 0.7%; Si: 0.01 to 0.8%; Mn: 0.1 to 1.5%; S: not more than 0.005%; P: not…
A low-alloy steel is produced through a process of in the smelting of low-alloy steel of composition comprising 0.1 to 0.55% C, 0.05 to 0.5% Si, 0.1 to 1% Mn, 0.0001 to 0.005% S, 0.005 to 0.08% Al, 0.005 to 0.05% Ti, 0.1 to 1.5% Cr, 0.1 to 1% Mo, 0.0004 to 0.005% O, 0.0005 to…
A steel for a steel pipe which has a chemical composition that C: 0.2 to 0.7 %, Si: 0.01 to 0.8 %, Mn: 0.1 to 1.5 %, S: 0.005 % or less, P: 0.03 % or less, Al: 0.0005 to 0.1 %, Ti: 0.005 to 0.05%, Ca: 0.0004 to 0.005 %, N: 0.007 % or less, Cr: 0.1 to 1.5 %, Mo: 0.2 to 1.0 %, Nb:…
A method of smelting a highly clean steel with extremely low sulfur content, involving treating of molten steel through the following steps (1) to (4). Step (1): a CaO-based flux is added to the molten steel within a ladle under atmospheric pressure. Step (2): an agitation gas…
A steel for steel pipes excellent in sour resistance which contains C, Mn, Si, P, S, Ti, Al, Ca, N, O and, if necessary, one or more of Cr, Ni, Cu, Mo, V, B and Nb in prescribed amounts, in which the inclusion of the steel comprises Ca, Al, O and S as the main components and in…
A low alloy steel, which has a chemical composition by mass %, of C: 0.1 to 0.55%, Si: 0.05 to 0.5%, Mn: 0.1 to 1%, S: 0.0001 to 0.005%, Al: 0.005 to 0.08%, Ti: 0.005 to 0.05%, Cr: 0.1 to 1.5%, Mo: 0.1 to 1%, O: 0.0004 to 0.005%, Ca: 0.0005 to 0.0045%, Nb: 0 to 0.1%, V: 0 to…
A process for producing an extra-low-sulfur low-nitrogen high-cleanliness steel which comprises treating a molten steel through the following steps (1) to (3). Step 1 comprises adding a CaO flux to a molten steel in a ladle at atmospheric pressure. Step 2 comprises setting a…
To provide an oil-well steel pipe having excellent SSC resistance. The oil-well steel pipe according to the present invention contains, by mass percent, C: 0.15 to 0.35%, Si: 0.1 to 0.75%, Mn: 0.1 to 1.0%, Cr: 0.1 to 1.7%, Mo: 0.1 to 1.2%, Ti: 0.01 to 0.05%, Nb: 0.010 to 0.030%,…
An ultralow-sulfur high-cleanliness steel having an [S] of 10 ppm or lower and a T.[O] of 40 ppm or lower is produced by a simple means without the need of adding CaF2 to a molten steel in a ladle or increasing the temperature of the steel being discharged from a converter. The…