A semi-conducting material being a non-oxide material or an already doped oxide material, wherein said material is doped with Manganese, Mn, and is ferromagnetic at least at one temperature in the range between room temperature and 500 K. Preferably, the Manganese doped material…
Nm Spintronics Ab
The present invention provides a detector for detecting ionising radiation comprising at least one detector arranged to be connected to a read-out arrangement for the reading-out and the evaluation of a signal from the detector, which detector comprises a carrier material and a…
A magnetic tunnel junction having a tunneling barrier layer, wherein the tunneling barrier layer comprises a diluted magnetic semiconductor having spin sensitivity. The magnetic tunnel junction according to the present invention may comprise a bottom lead coupled to a bottom…
A method is provided for producing a doped dilute ferromagnetic semiconductor material, by doping Zinc Oxide in bulk form with manganese to a maximum level of 5 atomic percent concentration. The material is preferably sintered at a maximum temperature of 650° C. The result of…
The invention provides a magnetic tunnel junction having a tunneling barrier layer wherein said tunneling barrier layer comprises a diluted magnetic semiconductor with spin sensitivity. The magnetic tunnel junction may according to the invention comprise a bottom lead coupled to…
A semi-conducting material, a method for producing the material, and ways of implementing the material, wherein said material is doped with Cu or CuO, and is ferromagnetic at least at one temperature in the range between -55 DEG C and 125 DEG C. Typically the material may…
A detector for detecting ionising radiation comprising at least one detector arranged to be connected to a read-out arrangement for the reading-out and the evaluation of a signal from the detector, which detector comprises a carrier material and a layer (4) comprising an active…
Method for producing a doped dilute ferromagnetic semiconductor material, by doping Zinc Oxide in bulk form with Manganese to a maximum level of 5 atomic percent concentration. The material is preferably sintered at a maximum temperature of 650 °C. The result of this process is…
본 발명은 터널링 배리어층을 갖는 자기 터널 접합부를 제공하며, 여기서, 터널링 배리어층은 스핀 민감성을 갖는 반자성 반도체를 포함한다. 본 발명에 따른 자기 터널 접합부는 반자성 반도체에 결합되는 하부 전극에 결합된 하부 리드을 포함할 수 있고, 상기 반자성 반도체는 상부 리드에 결합된 상부 전극에 결합되며, 여기서 상기 하부 전극은 비자성이다. 본 발명은 또한 본 발명에 따른 자기 터널 접합부를 활용하는 다양한 컴포넌트들 및 컴퓨터를 더 제공한다.
The invention provides a method to create ferromagnetism in a semiconductor comprising the steps of: 5 - choosing a suitable semiconductor material, - applying a metal layer onto said semiconductor material, thereby creating a magnetic semiconductor in the diffusion layer…
A method is provided for producing a doped dilute ferromagnetic semiconductor material, by doping Zinc Oxide in bulk form with manganese to a maximum level of 5 atomic percent concentration. The material is preferably sintered at a maximum temperature of 650° C. The result of…
Method for producing a doped dilute ferromagnetic semiconductor material, by doping Zinc Oxide in bulk form with Manganese to a maximum level of 5 atomic percent concentration. The material is preferably sintered at a maximum temperature of 650 °C. The result of this process is…
A method is provided for producing a doped dilute ferromagnetic semiconductor material, by doping Zinc Oxide in bulk form with manganese to a maximum level of 5 atomic percent concentration. The material is preferably sintered at a maximum temperature of 650° C. The result of…
A semi-conducting material being a non-oxide material or an already doped oxide material, wherein said material is doped with Manganese, Mn, and is ferromagnetic at least at one temperature in the range between room temperature and 500 K. Preferably, the Manganese doped material…
The invention provides a magnetic tunnel junction having a tunneling barrier layer wherein said tunneling barrier layer comprises a diluted magnetic semiconductor with spin sensitivity. The magnetic tunnel junction may according to the invention comprise a bottom lead coupled to…
A semi-conducting material, a method for producing the material, and ways of implementing the material, wherein said material is doped with Cu or CuO, and is ferromagnetic at least at one temperature in the range between -55°C and 125°C. Typically the material may comprise GaP…
A detector for detecting ionising radiation comprising at least one detector arranged to be connected to a read-out arrangement for the reading-out and the evaluation of a signal from the detector, which detector comprises a carrier material and a layer (4) comprising an active…
반도전성 재료, 상기 재료의 제작 방법, 상기 재료를 실행하는 방법으로서, 상기 재료는 Cu 또는 CuO로 도핑되며, -55℃ 내지 125℃ 사이 범위의 적어도 하나의 온도에서 강자성이다. 일반적으로 상기 재료는 GaP 또는 GaN을 포함한다.
비-산화물 재료 또는 이미 도핑된 산화물 재료인 반도전형 재료는 망간(Mn)으로 도핑되고, 실온 내지 500K 사이의 범위의 적어도 하나의 온도에서 강자성이다. 상기 망간 도핑된 재료는 5 at% 이하의 망간 농도를 갖는 것이 바람직하다.
The invention provides a magnetic tunnel junction having a tunneling barrier layer wherein said tunneling barrier layer comprises a diluted magnetic semiconductor with spin sensitivity. The magnetic tunnel junction may according to the invention comprise a bottom lead coupled to…
A detector for detecting ionising radiation having at least one detector arranged to be connected to a read-out arrangement for the reading-out and the evaluation of a signal from the detector. The detector has a carrier material and a layer having an active detector material…
The invention provides a method to create ferromagnetism in a semiconductor comprising the steps of: 5 - choosing a suitable semiconductor material, - applying a metal layer onto said semiconductor material, thereby creating a magnetic semiconductor in the diffusion layer…
A semi-conducting material being a non-oxide material or an already doped oxide material, wherein said material is doped with Manganese, Mn, and is ferromagnetic at least at one temperature in the range between room temperature and 500 K. Preferably, the Manganese doped material…