The removal of radium from acid-leached uranium mill tailings has been difficult due to its strong retention as mixed sulfates and in adsorbed forms. With this invention the leaching action of a complexing agent (reducing the free radium cation concentration in solution) is…
Nirdosh Inderjit
Ferric nitrate leaching at 75° C. is found to remove up to 97% of the uranium and 93% of the radium from ores occurring in the Elliot Lake area of Canada, after an initial flotation-separation of the sulfide minerals from the ore. In processes of the invention an aqueous acidic…
Ferric chloride leaching at temperatures in the range 47°-74° C. is found to remove up to 97% of the uranium from ores occurring in the Elliot Lake area of Canada, but radium removal was found to be poor due to the formation of sulphates from the sulphides present in the ore. In…
ABSTRACT OF THE DISCLOSURE Ferric nitrate leaching at 75°C is found to remove up to 97% of the uranium and 93% of the radium from ores occurring in the Elliot Lake area of Canada, after an initial flotation-separation of the sulfide minerals from the ore. In processes of the…
ABSTRACT OF THE DISCLOSURE Ferric chloride leaching at temperatures in the range 47-74°C is found to remove up to 97% of the uranium from ores occurring in the Elliot Lake area of Canada, but radium removal was found to be poor due to the formation of sulphates from the…
ABSTRACT OF THE DISCLOSURE The removal of radium from acid-leached uranium mill tailings has been difficult due to its strong retention as mixed sulfates and in adsorbed forms. With this invention the leaching action of a complexing agent (reducing the free radium cation…