US 3,773,504 A#1809183 Most Cited · 34 citations0.6/yr · PR 10.61ExpiredUS · Utility
Copper base alloy having wear resistance at high temperatures
Inventors: Niimi I, Kaneko Y, Komiyama Y, Uchiyama Y, Takeda YAssignee: Niimi I, Kaneko YFiled 1971-08-31 · Granted 1973-11-20

The present invention relates to copper base alloys having excellent seizure resistance and wear resistance at high temperatures containing copper as the principal constituent, and zinc (Zn), aluminum (Al), manganese (Mn), silicon (Si), chromium (Cr), and phosphorus (P) as alloy…

US 3,790,352 A#7313464 Most Cited · 13 citations0.2/yr · PR 3.60ExpiredUS · Utility
Sintered alloy having wear resistance at high temperature
Inventors: Hashimoto K, Ushitani K, Serino Y, Mitani S, Niimi IAssignee: Niimi I, Hashimoto KFiled 1972-01-11 · Granted 1974-02-05

The present invention relates to iron-base sintered alloys having excellent wear resistance at high temperatures, and more particularly to alloys adapted for fabricating valve seat rings of internal combustion engines. The alloys of the present invention are characterized by…

US 3,841,386 A#19052836 Most Cited · 5 citations0.1/yr · PR 3.48ExpiredUS · Utility
Method of joining a beryllium workpiece to light metals
Inventors: Hashimoto K, Kaneko Y, Komiyama Y, Niimi IAssignee: Niimi I, Hashimoto KFiled 1973-05-25 · Granted 1974-10-15

The joining of beryllium to light metals, such as magnesium and aluminum is performed according to the following method. The joining method according to this invention thus comprises the steps: A. DIPPING THE SOLID BERYLLIUM WORKPIECE IN A MOLTEN BATH OF COPPER OR COPPER ALLOY…

US 3,776,705 A#27547952 Most Cited · 3 citations0.1/yr · PR 2.60ExpiredUS · Utility
Sintered alloy having wear resistance at high temperature
Inventors: Ishihara K, Serino Y, Mitani S, Imanishi K, Hashimoto KAssignee: Niimi I, Hashimoto KFiled 1971-08-17 · Granted 1973-12-04

The present invention relates to sintered alloys having wear resistance at high temperature composed of 5 to 15 percent tin and 4 to 25 percent chromium, the balance being copper, and the alloy being sintered to more than 88 percent of theoretical density ratio.