WO 03,047,005 A2#10973204 Most Cited · 9 citations0.4/yr · PR 4.63PendingWO · Application
Manufacturing a solar cell with backside contacts
Inventors: Muenzer AdolfAssignee: Shell Solar Gmbh, Muenzer AdolfFiled 2002-11-26

Solar cell (1) comprising a silicon wafer (3) having a basic doping, a light-receiving front side (4) and a backside (6), which is provided with an interdigital semiconductor pattern, which interdigital semiconductor pattern comprises a first pattern of at least one first…

WO 2010/052565 A2#15321108 Most Cited · 7 citations0.4/yr · PR 1.73PendingWO · Application
Method for manufacturing a solar cell with a two-stage doping

Method for manufacturing a solar cell with a two-stage doping (88, 89) including the following method steps of forming (14, 48) an oxide layer (82), which can be penetrated by a first dopant, on at least one part of the surface of a solar cell substrate (80), of forming (16; 50)…

WO 2005/059469 A1#16892319 Most Cited · 6 citations0.3/yr · PR 1.99PendingWO · Application
Measuring pyramid size on a textured surface
Inventors: Muenzer AdolfAssignee: Shell Solar Gmbh, Muenzer AdolfFiled 2004-12-10

A device for measuring the size of pyramids (3) on a textured surface (4) of an object (6), such as a photovoltaic element, which device (1) comprises an object holder (10), a light source (12) emitting during normal operation a beam of plane waves onto a region of the textured…

US 2013061924 A1#21670060 Most Cited · 5 citations0.4/yr · PR 1.35PendingUS · Application
Solar cell having dielectric back reflective coating and method for the production thereof

In a method for producing a solar cell, a layer stack of dielectric layers is applied to a back of a solar cell substrate and the layer stack is heated and is held at temperatures of at least 700° C. during a time period of at least 5 minutes. The novel solar cell has a layer…

WO 02,061,854 A2#21169133 Most Cited · 5 citations0.2/yr · PR 1.43PendingWO · Application
Method for structuring an oxide layer applied to a substrate material

The invention relates to a method for structuring an oxide layer applied to a substrate material. The aim of the invention is to provide an inexpensive method for structuring such an oxide layer. To this end, a squeegee paste that contains an oxide-etching component is printed…

WO 9,628,851 A1#19219037 Most Cited · 5 citations0.2/yr · PR 2.49PendingWO · Application
Solar cell with back surface field and process for producing it

For the simple production of a back surface field it is proposed that a boron-containing diffusion source layer (2) be applied to the rear (RS) of a silicon wafer (1) and boron be driven into the wafer to a depth of about 1 to 5 νm at 900 to 1200 °C. This is done in an…

US 2014051199 A1#29786640 Most Cited · 3 citations0.2/yr · PR 1.27PendingUS · Application
Method for producing silicon solor cells having a front-sided texture and a smooth rear side

Method for producing a silicon solar cell which is smoothly etched on one side, in which a front side and a rear side of a silicon substrate are etched ( 10 ) to form a smooth texture, a dielectric coating is then formed ( 14, 16 ) on the rear side of the silicon substrate and…

WO 2012/083944 A2#36251299 Most Cited · 2 citations0.1/yr · PR 1.18PendingWO · Application
Method for producing silicon solar cells having a front-sided texture and a smooth rear side surface

The invention relates to a method for producing a silicon solar cell which is smoothly etched on one side, in which a front and rear side of a silicon substrate are etched (10) to form a smooth texture, a dielectric coating is then applied onto the rear side of the silicon…

US 9,276,155 B2#51916911 Most Cited · 1 citations0.1/yr · PR 0.84ActiveUS · Utility
Solar cell having dielectric back reflective coating and method for the production thereof
Inventors: Muenzer Adolf, Teppe Andreas, Schoene Jan, Schlosser Reinhold, Keller SteffenAssignee: Muenzer Adolf, Teppe AndreasFiled 2011-03-03 · Granted 2016-03-01

In a method for producing a solar cell, a layer stack of dielectric layers is applied to a back of a solar cell substrate and the layer stack is heated and is held at temperatures of at least 700° C. during a time period of at least 5 minutes. The novel solar cell has a layer…

WO 2011/085715 A2#47231204 Most Cited · 1 citations0.1/yr · PR 0.99PendingWO · Application
Method for creating a two-stage doping in a semiconductor substrate

The invention relates to a method for creating a two-stage doping in a semiconductor substrate (80), wherein in a doping area (89) to be provided with the two-stage doping (90, 92), dopant is diffused into the semiconductor substrate (80) by means of heavy diffusion (10) and in…

US 10,115,851 B2#133462631 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Solar cell having a dielectric rear face coating and method for producing same
Inventors: Teppe Andreas, Muenzer Adolf, Schoene Jan, Hein Mathias, Winter PeterAssignee: Teppe Andreas, Muenzer AdolfFiled 2011-10-14 · Granted 2018-10-30

Solar cell (11; 21; 31) having a dielectric coating arranged on a back side of the solar cell (11; 21; 31) which is at least partly covered by at least one planar contact (12; 22; 32), a boundary line (14; 24; 34) of the at least one planar contact (12; 22; 32) having at least…

US 2013014819 A1#64785095 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for doping a semiconductor substrate, and solar cell having two-stage doping

A method for doping a semiconductor substrate includes heating the semiconductor substrate by irradiation with laser radiation and at the same time diffusing dopant from a dopant source into the semiconductor substrate in heated regions. The semiconductor substrate is heated by…

US 2013312823 A1#82446030 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Solar cell having a dielectric rear face coating and method for producing same

Solar cell ( 11; 21; 31 ) having a dielectric coating arranged on a back side of the solar cell ( 11; 21; 31 ) which is at least partly covered by at least one planar contact ( 12; 22; 32 ), a boundary line ( 14; 24; 34 ) of the at least one planar contact ( 12; 22; 32 ) having…

WO 02,061,854 A3#136622926 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Method for structuring an oxide layer applied to a substrate material
Inventors: Muenzer Adolf, Schlosser ReinholdAssignee: Shell Solar Gmbh, Muenzer AdolfFiled 2002-02-01

The invention relates to a method for structuring an oxide layer applied to a substrate material. The aim of the invention is to provide an inexpensive method for structuring such an oxide layer. To this end, a squeegee paste that contains an oxide-etching component is printed…

WO 03,047,005 A3#64165168 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Manufacturing a solar cell with backside contacts
Inventors: Muenzer AdolfAssignee: Shell Solar Gmbh, Muenzer AdolfFiled 2002-11-26

Solar cell (1) comprising a silicon wafer (3) having a basic doping, a light-receiving front side (4) and a backside (6), which is provided with an interdigital semiconductor pattern, which interdigital semiconductor pattern comprises a first pattern of at least one first…

WO 2005/081286 A1#71377873 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Device for applying a liquid dopant solution on a wafer
Inventors: Muenzer AdolfAssignee: Shell Solar Gmbh, Muenzer AdolfFiled 2005-02-11

Device (1) for applying a liquid dopant solution on a wafer (3), comprising a dopant distribution device (5), a rotatable horizontally translatable dopant-transfer roll (7) between a first roll position (15) and a second roll position, and a work table (9) for holding the wafer…

WO 2006/131526 A1#154486379 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Si solar cell and its manufacturing method
Inventors: Froitzheim Armin, Muenzer AdolfAssignee: Shell Solar Gmbh, Froitzheim ArminFiled 2006-06-07

A solar cell comprising a silicon body layer of n-type bulk doping having a front side and a rear side; a non-alloyed p-type doped region at the rear side of the body layer and forming a p/n-junction therewith; a rear side contact in electrical connection with the p-type doped…

WO 2009/033544 A1#127573195 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for annealing semiconductor components

A method for annealing semiconductor components comprises the following steps: providing a semiconductor component (1) comprising a semiconductor substrate (2) having at least one first contact structure (3) that has a screen printed contact from a first contact material, and at…

WO 2010/052565 A3#94243797 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for manufacturing a solar cell with a two-stage doping

Method for manufacturing a solar cell with a two-stage doping (88, 89) including the following method steps of forming (14, 48) an oxide layer (82), which can be penetrated by a first dopant, on at least one part of the surface of a solar cell substrate (80), of forming (16; 50)…

WO 2011/085715 A3#125986470 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for creating a two-stage doping in a semiconductor substrate

The invention relates to a method for creating a two-stage doping in a semiconductor substrate (80), wherein in a doping area (89) to be provided with the two-stage doping (90, 92), dopant is diffused into the semiconductor substrate (80) by means of heavy diffusion (10) and in…

WO 2011/107092 A2#131557483 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for doping a semiconductor substrate, and solar cell having two-stage doping

The invention relates to a method for doping a semiconductor substrate (50), wherein the semiconductor substrate (50) is heated by irradiation (14) with laser radiation (60) and at the same time dopant from a dopant source (54) is diffused (16) into the semiconductor substrate…

WO 2011/107092 A3#73525032 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for doping a semiconductor substrate, and solar cell having two-stage doping

The invention relates to a method for doping a semiconductor substrate (50), wherein the semiconductor substrate (50) is heated by irradiation (14) with laser radiation (60) and at the same time dopant from a dopant source (54) is diffused (16) into the semiconductor substrate…

WO 2011/107094 A2#124696302 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Solar cell having dielectric back reflective coating and method for the production thereof

The invention relates to a method for producing a solar cell (70), wherein a layer stack (74, 76) of dielectric layers (74, 76) is applied (14, 16; 54, 56) to a back of a solar cell substrate (72) and the layer stack (74, 75) is heated and is held (20) at temperatures of at…

WO 2011/107094 A3#142585455 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Solar cell having dielectric back reflective coating and method for the production thereof

The invention relates to a method for producing a solar cell (70), wherein a layer stack (74, 76) of dielectric layers (74, 76) is applied (14, 16; 54, 56) to a back of a solar cell substrate (72) and the layer stack (74, 75) is heated and is held (20) at temperatures of at…

WO 2012/083938 A2#142015106 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Solar cell having a dielectric rear face coating and method for producing same

The invention relates to a solar cell (11; 21; 31) comprising a dielectric coating (4) which is disposed on a rear face of the solar cell (11; 21; 31) and is covered at least partially by at least one flat contact (12; 22; 32), wherein a boundary line (14; 24; 34) of the at…