The invention relates to a method for operating a multi-cathode-PVD-coating system. According to the invention, one part of the cathodes operates after the high power impulse cathodic sputtering which is assisted by magnetic fields and the remainder operates after the direct…
Muenz Wolf-dieter
PVD process for coating substrates comprises pre-treating a substrate in the vapor produced by pulsed magnetic field-supported cathode sputtering. During the pre-treatment a magnetic field arrangement in the form of a magnetron cathode is used to support the magnetic field. The…
The apparatus includes a coating chamber, two or more cathodes which are arranged peripherally within the coating chamber, substrate carriers for holding the substrate, vacuum pumps and voltage sources wherein an individual anode is arranged centrally between the cathodes in the…
A cutting tool (10) for a machine tool has a substrate (20) and one or more coating layers (12-18) of materials with different Raman spectra, e.g. Tin, TiA1N, TiA1XN (where X = Y, Cr, Nb, W, Mo or the like), AlN, TiC, ZrN, TiZrN, CrN or VN. A Raman spectroscopic probe (22)…
A base for a decorative layer is provided comprising a first material capable of forming an anodic oxide and a second capable of forming an interference metal oxide formed on the first material. The material capable of forming an anodic oxide layer may comprise a barrier layer…
The invention relates to a PVD method and a PVD device for producing diamond-like (DLC) coatings with high adhesion and substrates coated according to the PVD method. The substrates which are to be coated are pretreated by means of high power impulse magnetron sputtering…
A method for coating and/or treating surfaces by means of high-power impulse magnetron sputtering (HIPIMS), is designed with a view to the most effective possible implementation of a sputtering process at low cost in such a way that at least two cathodes are pulsed…
High speed steel, hard metal and cermet tools, having an yttrium- and/or scandium-containing hard metal coating which has been heat treated, are new. High speed steel, hard metal and cermet tools have a coating of TiAlN, TiAlYN, TiAlCrYN, TiAlScN, TiAlCrScN, TiAlYScN or…
Disclosed are a device and a method for PVD coating substrates. The inventive device (1) comprises a coating chamber (2), two or several cathodes (3) that are peripherally disposed within the coating chamber, substrate supports (6) for retaining the substrates (4), vacuum pumps…
The invention relates to a method for operating a multi-cathode-PVD-coating system. According to the invention, one part of the cathodes operates after the high power impulse cathodic sputtering which is assisted by magnetic fields and the remainder operates after the direct…
Ternary hard material layers are described to which a small proportion of yttrium is added to increase the resistance to wear at elevated temperatures.
A method for producing a magnetic-field system for a cathode arrangement, wherein the cathode arrangement comprises one or more cluster magnetron cathodes, each having a plurality of part-segments and/or a plurality of DC-coupled individual cathodes, is designed with regard to…
Described is a process for coating brass with hard, multicolored layers using PVD techniques, involving nickel-free base metallization and an additional coating to provide decorative effects.
Described is a process for coating brass with hard, multicolored layers using PVD techniques, involving nickel-free base metallization and an additional coating to provide decorative effects.
The apparatus (1) comprises a coating chamber (2), two or more cathodes (3), which are arranged peripherally within the coating chamber, substrate carriers (6) for holding the substrate (4), vacuum pumps (8) and voltage sources (15, 16, 17, 18, 19) wherein an individual anode…
Production of corrosion resistant layers of niobium or tantalum on steel substrates comprises etching the substrate with niobium or tantalum ions before coating using a PVD process. The ions are produced by cathodic arc discharge. Preferred Process: Etching is carried out even…
PVD process for coating substrates comprises pre-treating a substrate in the vapor produced by pulsed magnetic field-supported cathode sputtering. During the pre-treatment a magnetic field arrangement in the form of a magnetron cathode is used to support the magnetic field. The…
Once a coating has been applied to tools, especially those containing Y, Sc, La or mixtures thereof, said tools undergo thermal treatment at temperatures ranging from 700-1100 °C during periods of approximately 0.5-10 hours.
The invention concerns in particular the use of a basic electrode made from a TiAl alloy containing between 15 and 80 atomic % Al in conjunction with the production of tantalum-like thin-film capacitors and/or electrolytic capacitors.
Disclosed are a device and a method for PVD coating substrates. The inventive device (1) comprises a coating chamber (2), two or several cathodes (3) that are peripherally disposed within the coating chamber, substrate supports (6) for retaining the substrates (4), vacuum pumps…
The invention concerns in particular the use of a basic electrode made from a TiAl alloy containing between 15 and 80 atomic % Al in conjunction with the production of tantalum-like thin-film capacitors and/or electrolytic capacitors.