The thin flat glass substrate, especially for display engineering, has a thickness of less than 1.5 mm, a length of at least 1800 mm, a width of at least 1800 mm and a difference between a smallest thickness and largest thickness of less than 50 μm. The float glass process for…
Morstein Andreas
In the method for cutting a continuous glass sheet during production of flat glass with an inhomogeneous thickness distribution across a width of the glass sheet, a cutting tool is moved at an angle to a travel direction of the glass sheet across its width with a cutting force…
In the method for cutting a continuously moving glass sheet with an inhomogeneous thickness distribution across the glass sheet, a cutting tool is moved across it at an angle to its travel direction to form a fissure and then the glass sheet is broken along the fissure. To avoid…
The invention relates to a roller-equipped annealing lehr for flat glass ( 1 ), having a roller conveyor, which is accommodated inside a lehr housing, and having heating units ( 2 ) that are arranged in pairs above and below the roller conveyor, in rows situated one after…
The thin flat glass substrate, especially for display engineering, has a thickness of less than 1.5 mm, a length of at least 1800 mm, a width of at least 1800 mm and a difference between a smallest thickness and largest thickness of less than 50 μm. The float glass process for…
In the method for cutting a continuously moving glass sheet with an inhomogeneous thickness distribution across the glass sheet, a cutting tool is moved across it at an angle to its travel direction to form a fissure and then the glass sheet is broken along the fissure. To avoid…
As a result of production, these glass sheets (1), at the sides of the sheet, i.e. the so-called borders, have a different glass thickness than in the so-called net area. The continuous glass sheet (1, 1') is severed in a cross cutter (2) at the end of the cooling process,…
The invention relates to a device for the production of flat glass by the float method with a float chamber and several serially-arranged gap seals, whereby the last gap seal in the direction of travel of the strip, arranged at the glass outlet end, is separated from the ambient…
The invention relates to a method for reducing surface defects during production of a float glass with a transformation temperature Tg equal to or greater than 600 °C consisting in removing impurities from the surface of a glass strip in a float chamber by a molten metal flowing…
The invention relates to a method for reducing surface defects during the production of float glass having a transformation temperature Tg of at least 600 °C. The invention also relates to a method wherein impurities are removed from the surface of the glass band in the floating…
In the method for cutting a continuously moving glass sheet with an inhomogeneous thickness distribution across the glass sheet, a cutting tool is moved across it at an angle to its travel direction to form a fissure and then the glass sheet is broken along the fissure. To avoid…
The invention relates to a device for the production of flat glass by the float method with a float chamber and several serially-arranged gap seals, whereby the last gap seal in the direction of travel of the strip, arranged at the glass outlet end, is separated from the ambient…