A hermetically sealed glass package (100) and method (200) for manufacturing the hermetically sealed glass package (100) are described herein using an OLED display as an example. Basically, the hermetically sealed OLED display (100) is manufactured by providing (step 202) a…
Morena Robert M
A hermetically sealed glass package preform is provided comprising a glass substrate; a frit comprising 65 - 100 wt.% of a base glass and about 0 - 35 wt.% of a filler; wherein the base glass comprises: about 0 - 5 mole % K2O; about 0 - 35 mole % Sb2O3; about 0 - 20 mole % ZnO;…
A method of strengthening an alkali aluminoborosilicate glass. A compressive layer extending from a surface of the glass to a depth of layer is formed by exchanging larger metal cations for smaller metal cations present in the glass. In a second step, metal cations in the glass…
A solid oxide fuel cell device incorporates a sealing material resistant to hydrogen gas permeation at a sealing temperature in the intermediate temperature range of 600° C.-900° C., the seal having a CTE in the 100×10 −7 /° C. to 120×10 −7 /° C., wherein the sealing material…
A solid oxide fuel cell device incorporates a sealing material resistant to hydrogen gas permeation at a sealing temperature in the intermediate temperature range of 600° C.-800° C., the seal having a CTE in the 100×10 −7 /° C. to 120×10 −7 /° C., wherein the sealing material…
A dry glass-based fit, and methods of making a dry glass fit are disclosed. In one embodiment a dry glass frit comprises vanadium, phosphorous and a metal halide. The halide may be, for example, fluorine or chlorine. In another embodiment, a method of producing a dry glass frit…
≤A silicate glass that is tough and scratch resistant. The toughness is increased by minimizing the number of non-bridging oxygen atoms in the glass. In one embodiment, the silicate glass is an aluminoborosilicate glass in which -15 mol%≤ (R2O + R'O - Al2O3 - ZrO2) - B2O3 ≤…
The invention is directed to a glass composition that can be used to make glass frits suitable for use in the manufacturing of microreactors. The glass compositions, after final sintering to produce a finished microreactor, have a surface crystalline layer of 30 μm or less, or…
An antimony-free glass suitable for use in a frit for producing a hermetically sealed glass package is described. The hermetically sealed glass package, such as an OLED display device, is manufactured by providing a first glass substrate plate and a second glass substrate plate…
The invention is directed to a birefringent glass having a R 2 O—Al 2 O 3 —B 2 O 3 —SiO 2 base composition, where R 2 O represents alkali metal oxides, and a precipitated silver halide phase with a volume fraction of at least 0.001. The birefringent glass composition of the…
A method of forming an opal layer on an optically transparent alkali-silicate glass sheet, wherein a liquidus viscosity of the alkali silicate glass forming the sheet is at least about 200,000 poise, a liquidus temperature of the alkali silicate glass is equal to or less than…
Described herein are methods for making microfluidic devices comprising glass or glass-containing materials, wherein the methods have decreased cost and/or improved dimensional properties over similar formed glass articles produced using current techniques. In particular, a…
An antimony-free glass suitable for use in a frit for producing a hermetically sealed glass package is described. The hermetically sealed glass package, such as an OLED display device, is manufactured by providing a first glass substrate plate and a second glass substrate plate…
Strengthened glass substrates with glass fits and methods for forming the same are disclosed. According to one embodiment, a method for forming a glass frit on a glass substrate may include providing a glass substrate comprising a compressive stress layer extending from a…
Glasses having a low softening point and high toughness. The glasses are alkali aluminoborosilicate glasses having softening points of less than 900°C and, in some embodiments, in a range from about 650°C up to about 825°C, and an indenter damage threshold of at least 300 g for…
A system, method, and ink for printing a data carrying mark on a green ceramic honeycomb structure is provided. The system includes a printer having an ink jet print head that prints a mark, preferably in the form of a two-dimensional data matrix barcode, on a side wall of the…
A system, method, and ink for printing a data carrying mark on a green ceramic honeycomb structure is provided. The system includes a printer having an ink jet print head that prints a mark, preferably in the form of a two-dimensional data matrix barcode, on a side wall of the…
An antimony-free glass suitable for use in a frit for producing a hermetically sealed glass package is described. The hermetically sealed glass package, such as an OLED display device, is manufactured by providing a first glass substrate plate and a second glass substrate plate…
A system, method, and ink for printing a data carrying mark on a green ceramic honeycomb structure is provided. The system includes a printer having an ink jet print head that prints a mark, preferably in the form of a two-dimensional data matrix bar code, on a side wall of the…
Glass-bonded ceramics made of non-microcracked non-oxide or oxide ceramic particles which are bound together by glass into a unitary non-microcracked structure are disclosed. Such ceramics are suitable for use in substrates and filters, such as a diesel particulate filter.
According to one embodiment a solid oxide fuel cell device incorporates a seal resistant to hydrogen gas permeation at a in the range of 600°C to 9000C, the seal having a CTE in the 100xl0-7/°C to 120xl0-7/°C, wherein the seal includes a sealing material that comprises in weight…
A hermetically sealed glass package and method for manufacturing the hermetically sealed glass package are described herein using an OLED display as an example. In one embodiment, the hermetically sealed glass package is manufactured by providing a first substrate plate and a…
A micro fluidic device (10) comprises one or more fluidic passages or channels or chambers (26, 28) having one or more dimensions in the millimeter to sub-millimeter range, wherein the device (10) further comprises a consolidated mixture comprising a glass frit and a filler (20,…
The disclosure is directed to glass frits materials containing phosphors that can be used in LED lighting devices and for methods associated therewith for making the phosphor containing frit materials. Suitable non-lead glasses have a composition, in mol%, in the range of 20-24%…
Methods for molding glass and glass composites, including providing a first structure having a first surface, providing a second structure having a second surface, the second surface being patterned and porous, and disposing between the first and second surfaces an amount of a…