Paper, fabric, wood, glass, metal, and like materials are coated or impregnated with a solid polymer of ethylene by treatment with a solution or suspension of the polymer, by application of a melt of the polymer or by application of a pre-formed film of the polymer (with the aid…
Michael Willcox Perrin
Solid polymers of ethylene are produced (a) by subjecting ethylene, compressed to a pressure of at least 1200 ats., to a temperature of 100--300 DEG C., the temperature in any part of the gas being prevented from reaching that at which explosive decomposition occurs, or (b) by…
High molecular weight compounds are prepared by subjecting ethylene, in the presence of one or more other organic compounds containing one or more double bonds and capable of forming dimers or higher polymers, to a pressure of at least 500 atmospheres and a temperature of 100 to…
Solid ethylene polymer (which may contain a small amount of oxygen) is shaped at a temperature above its softening temperature, i.e. above about 110 DEG C., solidified by cooling and rolled or cut into one or more thin strips or sheets. The polymer, which may be prepared…
527,763. Electric cables. SWALLOW, J. C., PERRIN, M. W., and IMPERIAL CHEMICAL INDUSTRIES, Ltd. Feb. 2, 1939, No. 3519. Drawings to Specification..[Class 36] In an electric cable used for submarine telephony having two co-axial conductors, the space between them is completely…
Artificial threads are obtained by extruding or drawing a solid ethylene polymer in fluid form under such conditions that the material solidifies immediately it becomes attenuated. The material to be spun may be in molten form or in the form of a hot concentrated solution in a…
Articles are prepared from solid polymers of ethylene, with or without the addition of fillers, opacifying or colouring materials, by injection moulding.ALSO:Articles are prepared from solid polymers of ethylene, with or without the addition of fillers, opacifying or colouring…
528,970. Impregnating - compositions for electric insulation. WILLIAMS, E. G., SWALLOW, J. C., PERRIN, M. W., and IMPERIAL CHEMICAL INDUSTRIES, Ltd. May 4, 1939, No. 13395. [Class 140] [Also in Groups XXXVI and IV] A cable suitable for voltages up to 1,000 volts comprises a…
Drying-oils and fatty acids are polymerized by heating under pressure exceeding 500 atmos. Pressures up to 12,000 atmos. are specified. The oils and acids may first be de-gassed to remove water and dissolved oxygen; the products may be freed from p decomposed matter and from…
505,761. Cables. SWALLOW, J. C., PERRIN, M. W., and IMPERIAL CHEMICAL INDUSTRIES, Ltd. Oct. 14, 1937, No. 28020. [Class 36] A high frequency cable comprises two coaxial conductors spaced apart by insulating material occupying part of the annular space between the conductors,…