The invention relates to carbon black having a C-14 content greater than 0.05 Bq/g and a ratio ΔD50/Dmode of the aggregate size distribution of less than 0.7. The carbon black is produced by thermal oxidative pyrolysis or thermal cleavage of the carbon black raw material in that…
Assignee / Organization
Messer Paul
28Total Forward Citations
8Indexed Patents
4Avg Citations / Patent
3Portfolio H-Index
The invention relates to a rubber mixture comprising at least one rubber and at least one low-PAH-content carbon black, where the low-PAH-content carbon black has (A) an iodine number of from 17 to 75 mg/g, (B) an STSA surface area of from 17 to 64 m 2 /g, (C) an iodine…
The invention relates to carbon black having a C-14 content greater than 0.05 Bq/g and a ratio ΔD50/Dmode of the aggregate size distribution of less than 0.7. The carbon black is produced by thermal oxidative pyrolysis or thermal cleavage of the carbon black raw material in that…