Retaining piece for holding together two pieces of bone (20a, 20b) separated by a fracture (25) is formed from a metal having an austenite/martensite transition temp. close to ambient. The piece comprises an active section (1), between the contact zones (2a, 3a) of the bone,…
Memometal Ind
A holder, designed to support an osteosynthesis staple with at least two parallel pointed tips (3, 4), has a fork-shaped end with three prongs (6, 7, 8) and two gaps (10, 11) for the staple tips to pass through. The central prong of the holder is more rigid than the other two,…
A process for the production of a superelastic material out of a nickel and titanium alloy, characterized by the fact that it consists in obtaining an ingot starting from a mixing of nickel and titanium consisting in 55.6%±0.4% in weight of nickel and to proceed with a thermal…
Support (1) pour agrafe de contention ou d'ostéosynthèse (2), ladite agrafe étant pourvue d'au moins deux pattes (3, 4) sensiblement parallèles destinées à pénétrer dans un os, caractérisé en ce que ledit support est apte à supporter ladite agrafe en maintenant libres…
New Ni/Ti alloy (I) fixation or bone-grafting pin (II), where (I) has an austenite end-point temperature (Afo) in the absence of mechanical constraint of about 40-45 deg C. Also claimed is a method (III) of preparing (II), comprising preparing a bar of (I) comprising 55.3\!0.3…
Procédé de fabrication d'une pièce superélastique en alliage de nickel et de titane, caractérisé en ce qu'il consiste à réaliser un lingot (1, 2, 3) à partir d'un mélange de nickel et de titane comprenant 55,6% ± 0,4% en poids de nickel et à procéder à un traitement…
A holder, designed to support an osteosynthesis staple with at least two parallel pointed tips (3, 4), has a fork-shaped end with three prongs (6, 7, 8) and two gaps (10, 11) for the staple tips to pass through. The central prong of the holder is more rigid than the other two,…
The osteosynthesis pin consists of a cannula (2) of a malleable material, such as annealed stainless steel, with its tip (2b) cut at an angle to facilitate bone penetration. The outer diameter of the cannula is between 1 and 5 mm and preferably 1 - 3 mm, while its inner diameter…
Making nickel titanium alloy wire containing 55.2-56 wt.% nickel, comprises giving a final heating at 480-520 deg C for 5-60 minutes in order to generate platelets of martensite, conferring superelastic properties. Preferably the alloy is formed into an ingot that is repeatedly…
An object holder made of metal wire, especially a key ring, is produced from a shape memory alloy of e.g. nickel and titanium. Preferred alloys have a martensitic transformation start temperature of 0-20 (preferably 5-15) deg C, so that the easily deformable martensitic…
L'agrafe de l'invention est constituée par une canule (2) en matériau malléable qui peut être écrasée et appliquée à la périphérie de l'os (1).Une broche rigide (3) apte à être coiffée par la canule (2) est utilisée pour la mise en place de l'extrémité antérieure…
The accessory comprises a device for fixing to a motorized rotating tool (12) the driving end (18) of the screw (30). The accessory has an axial stop surface (44) able to be supported against a bone (46) during placing of the screw. This surface extends near to the fixing end.