The method comprises producting a linear coil (4) by winding around a cylindrical mandrel (5) a conductor wire coated with a thermo-adhesive varnish, opening the toroidal magnetic circuit (1), withdrawing the linear coil (4) from the cylindrical mandrel (5), heating the linear…
Mecagis
A device is provided for measuring electric current having at least one probe sensitive to magnetic flux arranged in the air gap of an annular core through which at least one conductor of a current to be measured is intended to pass. A compensation winding is wound of the core…
Process for manufacturing a magnetic component made of an iron-based soft magnetic alloy having a nanocrystalline structure, the chemical composition of which is, in at. %, Fe≧60%, 0.1%≦Cu≦3%, 0%≦B≦25%, 0%≦Si≦30%, and at least one element selected from niobium, tungsten,…
The present invention relates to a process of manufacturing magnetic components with fe-based soft magnetic alloy of nano-crystalline structure. The process comprises the following steps: magnetic alloy is used for manufacturing amorphous ribbons; the ribbons are used for…
Process for manufacturing at least one magnetic core made of an iron-based soft magnetic alloy having a nanocrystalline structure, wherein an amorphous ribbon is manufactured from the magnetic alloy, the annealing temperature Tm which, in the case of the ribbon, leads to maximum…
Process for the heat treatment, in a magnetic field, of a magnetic component made of a low-anisotropy soft magnetic material such as, for example, a 15/80/5 FeNiMo alloy, an amorphous Co-based alloy or a nanocrystalline FeSiCuNbB alloy, in which the magnetic component is…
The subject of the present invention is a mechanical damping device for a magnetic core (2) housed in a casing (3) formed of two half-casings (3a, 3b) and on which are wound several coils. The device includes elastic means (12) for fastening the magnetic core (2) to at least one…
Process for manufacturing at least one magnetic core made of an iron-based soft magnetic alloy having a nanocrystalline structure, wherein an amorphous ribbon is manufactured from the magnetic alloy, the annealing temperature Tm which, in the case of the ribbon, leads to maximum…
Device for producing a signal representative of the relative displacement of two elements with respect to each other, comprising an encoded target (reference marker) (1) solidly attached to one of the elements, and a magnetic sensor (3) for reading the code, solidly attached to…
Process for manufacturing a magnetic component made of an iron-based soft magnetic alloy having a nanocrystalline structure, according to which an amorphous ribbon is manufactured from the magnetic alloy, a blank for a magnetic component is manufactured from the ribbon and the…
A magnetisable material such as an iron-nickel-molybdenum 15-80-5 alloy, an amorphous cobalt-based alloy or an iron-silicon-copper-niobium-boron nanocrystalline alloy is heated below the Curie point. It is subjected to a magnetic field whose intensity is varied over time,…
Process for the heat treatment, in a magnetic field, of a magnetic component made of a low-anisotropy soft magnetic material such as, for example, a 15/80/5 FeNiMo alloy, an amorphous Co-based alloy or a nanocrystalline FeSiCuNbB alloy, in which the magnetic component is…
Production of a nanocrystalline soft magnetic iron-silicon-boron alloy magnetic core involves crystallization heat treatment of the amorphous alloy at 250-450 degrees C in a transverse magnetic field of rectangular waveform. Production of a magnetic core of nanocrystalline soft…
The production of a magnetic component from a nanocrystalline iron based soft magnetic alloy of composition (in at. %) ≥ 60 % Fe, 0.1-3 % Cu, 0-25 % B, 0-30 (preferably ≤ 14) % Si, 0.1-30 % one or more of Nb, W, Ta, Zr, high-frequency, Ti and Mo and balance impurities, the sum…
A device is provided for measuring electric current having at least one probe sensitive to magnetic flux arranged in the air gap of an annular core through which at least one conductor of a current to be measured is intended to pass. A compensation winding is wound of the core…
Production of a magnetic core of soft magnetic iron-based alloy having a nanocrystalline structure involves determining the annealing temperature (Tm) required, for an amorphous ribbon of the alloy, to achieve maximum magnetic permeability and subjecting a core blank, produced…
The production of a magnetic component from a nanocrystalline iron based soft magnetic alloy of composition (in at. %) ≥ 60 % Fe, 0.1-3 % Cu, 0-25 % B, 0-30 (preferably ≤ 14) % Si, 0.1-30 % one or more of Nb, W, Ta, Zr, high-frequency, Ti and Mo and balance impurities, the sum…
The relay has a permanent magnet (7) which provides an attractive force used to hold the armature (6) in place while a fault current through the coil (10) on the U-core acts to oppose the permanent field and allows displacement of the armature under the pull of a spring (8). The…
Production of a nanocrystalline soft magnetic iron-silicon-boron alloy magnetic core involves crystallization heat treatment of the amorphous alloy at 150-400 degrees C in a transverse magnetic field of rectangular waveform. Production of a magnetic core of nanocrystalline soft…
An electric current measuring device including at least one magnetic flux sensor (1) in the air gap (2) of a ring-shaped core (3) with at least one conductor (4) passing therethrough and carrying the current to be measured, a compensating winding (5) wound around the core (3),…
The process involves linearly winding the coil (4) around the toroidal magnetic circuit (1). The coil is then varnished with a thermo adhering varnish. The varnish is a polyurethane modified with polyester and a layer of polyamine. The toroid is then opened out, and the formed…
The relay has a permanent magnet (7) which provides an attractive force used to hold the armature (6) in place while a fault current through the coil (10) on the U-core acts to oppose the permanent field and allows displacement of the armature under the pull of a spring (8). The…
A device is provided for measuring electric current having at least one probe sensitive to magnetic flux arranged in the air gap of an annular core through which at least one conductor of a current to be measured is intended to pass. A compensation winding is wound of the core…
The electro-magnetic coupling of the two components (2, 3) is variable in terms of the relative position and the processing procedure (11) of an output signal from one of the electro-magnetic components (2), permitting the determination of the angular position of the rotating…
The optimum temperature of cooking oil in a frying vat is detected by a magnetic element whose Curic point temperature is slightly above the required value, and whose magnetic force acts against a speing. Two elements may be employed to signal upper and lower limits of…