The instant disclosure is directed to a thermoplastic vulcanizate composition comprising a dynamically-cured rubber; from about 20 to about 300 parts by weight of a thermoplastic resin per 100 parts by weight rubber and from about 30 to about 250 parts by weight additional oil…
Mcdaniel Paul E
A thermoplastic elastomer formed by a process comprising the steps of dynamically vulcanizing a rubber within a mixture that includes the rubber, from about 10 to about 80 percent by weight of a thermoplastic resin based upon the total weight of the rubber and the thermoplastic…
A thermoplastic vulcanizate comprising a dynamically-cured rubber, and a thermoplastic resin, where the rubber has been cured with a peroxide in the presence of a coagent selected from the group consisting of a high-vinyl polydiene, high-vinyl polydiene copolymer,…
A process for preparing a thermoplastic vulcanizate, the process comprising: charging a reactor with an olefmic copolymer rubber, where the olefmic copolymer rubber is characterized by a multimodal molecular weight, an average branching index of greater than 0.8, includes less…
A method for preparing a nanoclay-filled thermoplastic vulcanizate, the method comprising introducing an olefinic thermoplastic vulcanizate, a functionalized thermoplastic resin, and a surface-modified nanoclay, where the blending takes place at a temperature above the melt…
The instant disclosure is directed to a thermoplastic vulcanizate composition comprising a dynamically-cured rubber; from about 20 to about 300 parts by weight of a thermoplastic resin per 100 parts by weight rubber and from about 30 to about 250 parts by weight additional oil…
The disclosure is directed to a thermoplastic vulcanizate composition comprising a dynamically-cured rubber; from about 20 to about 300 parts by weight of a thermoplastic resin per 100 parts by weight rubber and from about 30 to about 250 parts by weight additional oil per 100…
A process for preparing a thermoplastic vulcanizate, the process comprising: charging a reactor with an olefinic copolymer rubber, where the olefinic copolymer rubber is characterized by a multimodal molecular weight, an average branching index of greater than 0.8, includes less…
A thermoplastic vulcanizate comprising a dynamically-cured rubber, and a thermoplastic resin, where the rubber has been cured with a peroxide in the presence of a coagent selected from the group consisting of a high-vinyl polydiene, high-vinyl polydiene copolymer,…
The disclosure is directed to a thermoplastic vulcanizate composition comprising a dynamically-cured rubber; from about 20 to about 300 parts by weight of a thermoplastic resin per 100 parts by weight rubber and from about 30 to about 250 parts by weight additional oil per 100…