A sulfonated gilsonite used in a drilling mud for drilling a well wherein the sulfonated gilsonite is prepared by reacting at a temperature between 210 DEG -280 DEG F. with a mixture of water, gilsonite having a softening point of at least 300 DEG F., lignite, sulfonating…
Assignee / Organization
Mccrary Jack L
15Total Forward Citations
1Indexed Patents
15Avg Citations / Patent
1Portfolio H-Index
Key Inventors: Mccrary Jack L