A method of fabricating aluminum alloys containing finely dispersed aluminum-transition metal intermetallic phases is disclosed. The alloys are subjected to melt spinning to form a brittle filament consisting in large measure of a metastable face-centered cubic solid solution;…
Marko Materials Inc
Alloys, of iron, cobalt, nickel and chromium containing both metalloids and refractory metals are disclosed. The alloys are rapidly solidified at cooling rates of 10 5 -10 7 ° C./sec so as to produce an ultrafine grained metastable crystal structure having enhanced compositional…
Alloys having compositions similar to commercial tool steels, but modified by the addition of 0.1 to 1.5 wt. % boron are disclosed. The alloys are subjected to a rapid solidification processing (RSP) technique, producing cooling rates between 10 5 -10 7 °C./sec. The as-quenched…
Nickel and iron-nickel base alloys are described together with a rapid solidification process used in the preparation thereof to provide materials useful in the fabrication of parts subject to high temperature operating conditions. The alloys include commercial nickel base…
Iron base alloys containing chromium and refractory metals as well as 0.8 to 1.3 wt % boron are disclosed. The alloys are subjected to a rapid solidification processing (RSP) technique, producing cooling rates of about 10 5 to 10 7 ° C./sec. The as-quenched RSP ribbon, or…
New nickel and cobalt base alloys containing tungsten and carbon are disclosed. The alloys are subjected to rapid solidification processing (RSP) technique which produces cooling rates between 105 DEG to 107 DEG C./sec. The as-quenched ribbon, powder, etc. consists predominantly…
New iron base alloys containing aluminum and boron are disclosed. The alloys are subjected to a rapid solidification processing (RSP) technique which produces cooling rates between ˜10 5 to 10 7 ° C./sec. The as-quenched ribbon or powder, etc consists primarily of a metastable…
Alloys having compositions similar to commercial tool steels, but modified by the addition of 0.1 to 1.5 wt% boron are subjected to a rapid solidification processing (RSP) technique, producing cooling rates between 10<5>-10<7> DEG C/sec. The asquenced RSP ribbon or…
Nickel-aluminum alloys containing boron in powder form are disclosed. These alloys are subjected to melt-spinning to form a brittle filament consisting in large measure of a metastable solid solution phase. This is then pulverized to powder configuration. Such powders exhibit…
New iron rich metal alloys containing aluminum and copper along with specific amounts of boron are disclosed. The alloys are subjected to rapid solidification processing (RSP) technique which produces cooling rates between ˜10 5 to 10 7 °C./sec. The as-quenched ribbon, powder…
Alloys having composition similar to commercial precipitation-hardenable stainless steels, but modified by the addition of 1.4 to 2.4 wt % boron, are disclosed. The alloys are subjected to a rapid solidification processing (RSP) technique which produces cooling rates between ˜10…
New copper-rich metal alloys containing nickel along with certain specific amounts of boron are disclosed. The alloys are subjected to a rapid solidification processing (RSP) technique which produces cooling rates between ˜10 5 ° to 10 7 ° C./sec. The asquenched ribbon, powder,…
New nickel rich metal alloys containing copper along with specific amounts of boron are disclosed. The alloys are subjected to rapid solidification processing (RSP) techniques which produce cooling rates between ˜10 5 ° to 10 7 ° C./sec. The as-quenched ribbon, powder, etc.…
New cobalt base alloys containing chromium and carbon are disclosed. The alloys are subjected to rapid solidification processing (RSP) technique which produces cooling rates between 105 to 107oC/sec. The as-quenched ribbon, powder etc. consists predominantly of amorphous phase.…
The alloy has the general compsn. (by wt) 0.2-1.8 (pref. 0.5-1.6)%C, 0-20 (pref. 0-5)% Cr, 0-20 (pref. 0-6)% V, 0-20 (pref. 0-10)%Mo, 0-30 (pref. 0-20)% W, 0-20 (pref. 0-15)% Co, less than 2% Mn+Si+Ni, balance Fe and impurities, with the addn. of 0.1-1.5 (pref. 0.2-1)%B. The…