US 2011318982 A1#3958887 Most Cited · 21 citations1.4/yr · PR 3.26PendingUS · Application
Liquid crystal polyester fibers and method for producing the same

Disclosed are liquid crystal polyester fibers, which have a peak half-width of 15° C. or greater at an endothermic peak (Tm1) observed by differential calorimetry under a temperature elevation of 20° C./minute from 50° C., polystyrene equivalent weight average molecular weight…

WO 2008/105439 A1#7938091 Most Cited · 12 citations0.7/yr · PR 5.32PendingWO · Application
Liquid crystalline polyester fiber and process for production of the same

A liquid crystalline polyester fiber which exhibits a half width of endothermic peak (Tm1) of 15°C or above as observed in the differential calorimetry under heating from 50°C at a temperature rise rate of 20°C/min and a tenacity of 12.0cN/dtex or above; and a process for…

WO 2010/007919 A1#9191708 Most Cited · 11 citations0.7/yr · PR 2.45PendingWO · Application
Polyphenylene sulfide fiber, process for producing the same, wet-laid nonwoven fabric, and process for producing wet-laid nonwoven fabric

Polyphenylene sulfide fibers which are amorphous, have a low degree of thermal shrinkage, and are suitable for use as a binder for papermaking, etc.; a process for producing the fibers; a wet-laid nonwoven fabric comprising the polyphenylene sulfide fibers; and a process for…

WO 2010/103986 A1#9070130 Most Cited · 11 citations0.7/yr · PR 2.71PendingWO · Application
Liquid crystal polyester fibers and method for producing the same

Provided are liquid crystal polyester fibers, which have a peak half-width of 15°C or greater at an endothermic peak (Tm1) observed by differential calorimetry under a temperature elevation rate of from 50 to 20°C/minute, a weight-average molecular weight in terms of polystyrene…

US 2010104870 A1#11045815 Most Cited · 9 citations0.6/yr · PR 3.52PendingUS · Application
Liquid crystalline polyester fiber and process for production of the same

A liquid crystalline polyester fiber which exhibits a half width of endothermic peak (Tm1) of 15° C. or above as observed in differential calorimetry under heating from 50° C. at a temperature elevation rate of 20° C./min and a strength of 12.0 cN/dtex or more; and a process for…

US 8,101,688 B2#16183212 Most Cited · 7 citations0.5/yr · PR 1.22ActiveUS · Utility
Polylactic acid fiber yarn package, and textile products
Inventors: Kimura Toshiaki, Nonaka Shuichi, Ochi Takashi, Mihara Takaaki, Mochizuki KatsuhikoAssignee: Kimura Toshiaki, Nonaka ShuichiFiled 2011-01-03 · Granted 2012-01-24

Polylactic acid fibers excellent in wearing resistance and in the ability to smoothly pass through processing steps. The polylactic acid fibers contain a fatty acid bisamide and/or an alkyl-substituted fatty acid monoamide in an amount of 0.1 to 5 wt. % based on the whole fibers.

WO 2004/020708 A1#17350405 Most Cited · 6 citations0.3/yr · PR 1.75PendingWO · Application
Polylactic acid fiber, yarn package, and textile product

Polylactic acid fibers excellent in wearing resistance and in the ability to smoothly pass through processing steps. The polylactic acid fibers contain a fatty acid bisamide and/or an alkyl-substituted fatty acid monoamide in an amount of 0.1 to 5 wt.% based on the whole fibers.

US 9,011,743 B2#26720897 Most Cited · 4 citations0.4/yr · PR 1.17ActiveUS · Utility
Liquid crystal polyester fibers and method for producing the same
Inventors: Funatsu Yoshitsugu, Maeda Yuhei, Suzuki Norio, Katsuta HirooAssignee: Funatsu Yoshitsugu, Maeda YuheiFiled 2010-03-04 · Granted 2015-04-21

Disclosed are liquid crystal polyester fibers, which have a peak half-width of 15° C. or greater at an endothermic peak (Tm1) observed by differential calorimetry under a temperature elevation of 20° C./minute from 50° C., polystyrene equivalent weight average molecular weight…

WO 2004/101871 A1#25595870 Most Cited · 4 citations0.2/yr · PR 1.29PendingWO · Application
Fiber excellent in magnetic field responsiveness and conductivity and product consisting of it
Inventors: Miyazono Kouki, Maeda YuheiAssignee: Toray Industries, Miyazono KoukiFiled 2004-05-18

A fiber which consists of polymer containing a spherical magnetic material with a saturation magnetic flux density of at least 0.5 Tesla and having a fiber forming capability, and which is excellent in magnetic field responsiveness and conductivity. In a preferable mode, (a) an…

US 2007176315 A1#36993029 Most Cited · 2 citations0.1/yr · PR 1.13PendingUS · Application
Process for producing woody molding

A method is provided for manufacturing a molded woody article. The method includes compression molding a base material containing wood fibers, polylactic acid fibers and an inorganic filler at a temperature not less than a melting point of said polylactic acid fibers, and…

US 2011165370 A1#39967349 Most Cited · 2 citations0.1/yr · PR 1.01PendingUS · Application
Polylactic acid fiber yarn package, and textile products

Polylactic acid fibers excellent in wearing resistance and in the ability to smoothly pass through processing steps. The polylactic acid fibers contain a fatty acid bisamide and/or an alkyl-substituted fatty acid monoamide in an amount of 0.1 to 5 wt. % based on the whole fibers.

WO 0,123,651 A1#36149637 Most Cited · 2 citations0.1/yr · PR 1.20PendingWO · Application
Polypropylene terephthalate twisted yarn and method for producing the same

A method for producing polypropylene terephthalate twisted yarns, characterized as comprising utilizing polypropylene terephthalate unstretched yarns and carrying out stretching and twisting at the same time under specific conditions; and polypropylene terephthalate twisted…

WO 0,136,724 A1#44344906 Most Cited · 2 citations0.1/yr · PR 0.91PendingWO · Application
Polyester yarn and method for production thereof

A multifilament yarn consisting essentially of polytrimethylene terephthalate, characterized in that a strength in a stress-strain curve of 3 cN/dtex or more, a Young's modulus of 25 cN/dtex or less, a minimum differential Young's modulus in the range of 3 to 10 %…

US 8,673,174 B2#61276179 Most Cited · 1 citations0.1/yr · PR 0.75ActiveUS · Utility
Liquid crystalline polyester fiber and process for production of the same
Inventors: Funatsu Yoshitsugu, Katsuta Hiroo, Maeda YuheiAssignee: Funatsu Yoshitsugu, Katsuta HirooFiled 2008-02-27 · Granted 2014-03-18

A liquid crystalline polyester fiber which exhibits a half width of endothermic peak (Tm1) of 15° C. or above as observed in differential calorimetry under heating from 50° C. at a temperature elevation rate of 20° C./min and a strength of 12.0 cN/dtex or more; and a process for…

WO 2005/087468 A1#53588572 Most Cited · 1 citations0.1/yr · PR 0.82PendingWO · Application
Process for producing woody molding

A process for producing a woody molding, comprising the molding step of performing compression molding of a base material containing a wood fiber, a polylactic acid fiber and an inorganic filler at temperature of ≥ melting point of the polylactic acid fiber; and the…

WO 2005/123996 A1#52081474 Most Cited · 1 citations0.1/yr · PR 0.83PendingWO · Application
Polyester fiber excelling in weight lightness

A polyester fiber excelling in weight lightness and fiber properties, such as strength, and being free from concern over yellowing. There is provided a polyester fiber comprising polyester (A) and polymer (B) incompatible with the polyester (A), having discontinuous voids in the…

US 8,734,614 B2#118672446 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Polyphenylene sulfide fiber, method for producing the same, wet-laid nonwoven fabric, and method for producing wet-laid nonwoven fabric
Inventors: Takano Tomoko, Sugano Koji, Maeda Yuhei, Sugimoto TakeshiAssignee: Takano Tomoko, Sugano KojiFiled 2009-07-08 · Granted 2014-05-27

A polyphenylene sulfide fiber has an amount of heat of crystallization measured by DSC is 10 J/g or more and the degree of shrinkage on dry heating of 150° C.×30 minutes is 20% or less. A method produces a densified wet-laid nonwoven fabric by subjecting paper produced in a…

WO 9,411,550 A1#139543162 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method and apparatus for producing polyester fiber

This invention relates to a method and an apparatus for producing a polyester fiber involving the steps of cooling a plurality of polyester fibers melt-spun from a spinneret (2) to a temperature below a glass transition point, taking up the fibers at a take-up speed of less than…