A method of producing a chilled iron camshaft from a chromium containing cast iron is described. The cast iron material contains between 0.5 wt % to 1.2 wt % of chromium. The camshaft having a white iron structure adjacent chill inserts in a casting mold and a grey iron…
Lydmet Ltd
A method of producing a chilled iron camshaft is described, wherein the iron has a white iron structure (22) adjacent chill inserts (14) in a casting mould (12) and a grey iron structure (24) in substantially all other regions remote from the chills. The method comprises the…
A method of producing a chilled iron camshaft is described, wherein the iron has a white iron structure adjacent chill inserts in a casting mould and a grey iron structure in substantially all other regions remote from the chills. The method comprises the steps of assembling a…
Cams for mounting on a shaft are manufactured by assembling a stack of dies 10 with frangible members 12 interposed therebetween, each of the dies 10 defining cam-shaped cavities 24 and the frangible members 12 defining restricted orifices 32 inter-connecting the adjacent…
A method of producing a chilled iron camshaft from a chromium containing cast iron is described. The cast iron material contains between 0.5 wt % to 1.2 wt % of chromium, the camshaft having a white iron structure adjacent chill inserts in a casting mould and a grey iron…
A method of producing a chilled iron camshaft from a chromium containing cast iron is described. The cast iron material contains between 0.5 wt % to 1.2 wt % of chromium, the camshaft having a white iron structure adjacent chill inserts in a casting mould and a grey iron…
ABSTRACT Camshafts A method of producing a chilled iron camshaft is described, wherein the iron has a white iron structure adjacent chill inserts in a casting mould and a grey iron structure in substantially all other regions remote from the chills. The method comprises the…
ABSTRACT A method of producing a chilled iron camshaft from a chromium containing cast iron is described. The cast iron material contains between 0.5 wt% to 1.2 wt% of chromium, the camshaft having a white iron structure adjacent chill inserts in a casting mould and a grey iron…
On décrit un procédé de fabrication d'un arbre à cames en fonte coulé en coquille à partir d'une fonte contenant du chrome. Le matériau en fonte contient entre 0,5 et 1,2 % en poids de chrome, l'arbre à cames présentant une structure de fonte blanche brute adjacente…
L'invention a pour but de remédier aux difficultés rencontrées pour la coulée de fonte à une température de 1000 degrés C à 1700 degrés C dans un moule en vue de l'obtention d'une pièce creuse dont la cavité intérieure est longue par rapport à sa dimension…
La presente invención se refiere a un método para producir un árbol de levas de hierro templado, el hierro tiene una estructura de hierro blanco adyacente a insertos para templado en un molde para fundido y una estructura de hierro gris en substancialmente todas las regiones…