High strength steel is produced by a first rolling of a steel composition, reheated above 1100° C., above the austenite recrystallization, a second rolling below the austenite recrystallization temperature, water cooling from above Ar 3 to less than 400° C. and followed by…
Assignee / Organization
Luton; Michael John
25Total Forward Citations
2Indexed Patents
12Avg Citations / Patent
1Portfolio H-Index
A method for refining the grain size of alloys which undergo ferromagnetic to paramagnetic phase transformation and an alloy produced therefrom. By subjecting the alloy to a timed application of a strong magnetic field, the temperature of phase boundaries can be shifted enabling…