The present invention generally relates to an improvement in the process for manufacturing optical fibers by drawing a preform made by vapour phase deposition techniques. More specifically, the present invention recognizes and obviates adverse effects on the operational…
Litespec Inc
In a VAD method for making optical fiber preforms, the yield is increased by terminating or significantly reducing the supply of glass raw material to the torch (24) just after glass jacket soot (23, FIG. 4) has been deposited at the bottom end of the glass rod (20). The fuel…
PURPOSE: To make it possible to drastically shorten a sintering and annealing time by only partially sintering a jacket soot boule in an inert gaseous atmosphere. CONSTITUTION: A glass core rod 20 is coated by the jacket soot boule 21. The jacket soot boule 21 is sintered by…
PROBLEM TO BE SOLVED: To improve the removal of metal impurities in an optical fiber and preform. SOLUTION: Clad glass soot having a second refractive index lower than a first refractive index is deposited on core glass having the first refractive index, by which a soot pool…
PURPOSE: To produce an optical fiber preform in a manner as not to crack a glass soot boule. CONSTITUTION: The supply of glass raw material 26 to a burner 24 is ended (or is rapidly lessened) right after glass jacket soot 23 deposits on the bottom end of a glass rod 27'. The…
In a VAD method for making optical fiber preforms, the yield is increased by terminating or significantly reducing the supply of glass raw material to the torch (24) just after glass jacket soot (23, FIG. 4) has been deposited at the bottom end of the glass rod (20). The fuel…
In a method for making optical fiber preforms, the time taken for sintering and annealing the clad or jacket layer is significantly reduced by only partially sintering the jacket soot boule in an atmosphere of helium. For example, instead of using one hundred forty-three minutes…