The method comprises (1) mixing 2-5 parts heat-stabilizer, 20-30 parts graphite powder, with 65-75 parts polyester in the mixer, (2) preheating the mixture in the extruder at 200 deg.C, melting at 220 deg.C, mixing at 220 deg.C, inserting copper wire at 200 deg.C and molding at…
Assignee / Organization
Lim Pil Sub
1Total Forward Citations
2Indexed Patents
0Avg Citations / Patent
1Portfolio H-Index
내용 없음.