US 2007246137 A1#4902338 Most Cited · 18 citations0.9/yr · PR 3.19PendingUS · Application
Method Of Making A Structural Element For Aeronautical Construction Comprising Differential Work-Hardening

A process for fabricating a worked product or a monolithic multi-functional structural element comprising aluminium alloy includes a hot working step and at least one transformation step by cold plastic deformation after the hot transformation step. At least two zones of the…

US 2005217770 A1#5178026 Most Cited · 17 citations0.8/yr · PR 4.23PendingUS · Application
Structural member for aeronautical construction with a variation of usage properties
Inventors: Lequeu Philippe, Dumont DavidAssignee: Lequeu Philippe, Dumont DavidFiled 2005-03-23

This invention relates to a process for manufacturing an aluminium alloy part with structural hardening as well as to structural members including monolithic structural members and to products prepared from such structural members. A suitable process of the present invention…

WO 2005/098072 A2#5753158 Most Cited · 16 citations0.8/yr · PR 3.00PendingWO · Application
Structural element for aircraft engineering exhibiting a variation of performance characteristics
Inventors: Lequeu Philippe, Dumont DavidAssignee: Pechiney Rhenalu, Lequeu PhilippeFiled 2005-03-21

The invention relates to a method for producing a part made of aluminium alloy with structural hardening consisting a) in melting a semifinished extruded or forged rolled stock followed by water quenching, b) in optionally carrying out a controlled drawing with a permanent…

US 2006151075 A1#6380543 Most Cited · 15 citations0.8/yr · PR 2.44PendingUS · Application
Low internal stress Al-Zn-Cu-Mg plates

The present invention relates to a method for producing Al—Zn—Cu—Mg type alloy plates comprising between 4 and 12% zinc, less than 4% magnesium and less than 4% copper, other elements≦0.5% each, and the remainder aluminum. The method comprising hot rolling, solution…

WO 2006/064113 A1#18093026 Most Cited · 6 citations0.3/yr · PR 1.52PendingWO · Application
High strength sheet made from al-zn-cu-mg alloy with low internal stresses

The invention relates to a method for production of thick sheets made from Al-Zn-Cu-Mg type alloys, comprising 4 to 12 % zinc, less than 4 % magnesium, less than 4 % copper, trace elements = 0.5 % each, the remainder being aluminium, said method comprising hot lamination,…

WO 2010/130887 A1#24898484 Most Cited · 4 citations0.2/yr · PR 1.36PendingWO · Application
Method for assembling parts made of an aluminum alloy by welding, comprising cold deformation followed by the post-welding tempering of the entire welded area

The invention relates to a method for assembling parts (14a, 14b) made of an aluminum alloy, comprising: (I) providing at least one first part (14a) made of an aluminum alloy and which has been put in a solution, tempered, optionally hammer-hardened, and naturally aged at…

WO 2007/080265 A1#43436495 Most Cited · 2 citations0.1/yr · PR 0.93PendingWO · Application
Process for manufacturing semi-finished products comprising two aluminium-based alloys

The invention relates to a process for the vertical casting of an intermediate product, comprising step (a) of preparing at least two aluminium-based alloys, especially a first alloy of composition P and a second alloy of composition T; step (b) of casting the first alloy of…

US 10,144,998 B2#81628823 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method of making a structural element for aeronautical construction comprising differential work-hardening
Inventors: Lequeu Philippe, Heymes Fabrice, Danielou ArmelleAssignee: Lequeu Philippe, Heymes FabriceFiled 2007-04-13 · Granted 2018-12-04

A process for fabricating a worked product or a monolithic multi-functional structural element comprising aluminium alloy includes a hot working step and at least one transformation step by cold plastic deformation after the hot transformation step. At least two zones of the…

US 8,469,255 B2#135952648 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for assembling aluminum alloy parts by welding

The present disclosure concerns a method for assembling aluminum alloy parts, in which (i) at least a first aluminum alloy part is procured in a solution heat treated, quenched, optionally cold worked, and naturally aged at ambient temperature or pre-aged temper, and at least a…

WO 2005/098072 A3#129487526 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Structural element for aircraft engineering exhibiting a variation of performance characteristics
Inventors: Lequeu Philippe, Dumont DavidAssignee: Alcan Rhenalu, Lequeu PhilippeFiled 2005-03-21

The invention relates to a method for producing a part made of aluminium alloy with structural hardening consisting a) in melting a semifinished extruded or forged rolled stock followed by water quenching, b) in optionally carrying out a controlled drawing with a permanent…

WO 2007/122314 A1#81704110 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for fabrication of a structural element for aeronautical construction including a differential work hardening

The invention relates to a method for manufacturing a work hardened product or a monolithic multifunctional structural element made of an aluminium alloy comprising a hot transformation step characterised in that after the hot transformation step, it also comprises at least one…