Chlorinated rubber giving solutions of low viscosity is made by heating rubber in air to 90-130 DEG C. for an extended period, with or without mastication, and then chlorinating or hydrochlorinating, preferably in solution, in e.g. carbon tetrachloride. The rubber is preferably…
Leonard Thane Dod
A chlorinated rubber containing 2-20 per cent of chlorine, is incorporated with a fully chlorinated rubber containing more than 55 per cent, preferably about 65 per cent of chlorine to obtain a product which is flame-resistant and plastic and elastic. The properties of the…
Electrical apparatus is insulated with a material obtained by chlorinating rubber until it contains not substantially more than 20 per cent of chlorine, and subsequently vulcanizing. Highly chlorinated rubber may be mixed with the lightly chlorinated rubber before vulcanization,…
Rubber is chlorinated until it contains up to 20 per cent of chlorine, and this product is vulcanized. The lightly chlorinated rubber may be mixed with fully chlorinated rubber as described in Specification 487,167, and this product vulcanized. Hot or cold vulcanization may be…