Calcium, magnesium barium, zinc, iron and aluminium orthophosphates are prepared by treating salts or oxides of these metals with phosphoric acid (which may be formed in situ) first at a temperature below 30 DEG C. and pH 1.5-2.5, then at above 60 DEG C. and pH 2.5-3.5,…
Kunio Taguchi
A quick-setting cement comprises a dehydrated metal dihydrogen phosphate and a metal oxide, where the metal may be zinc, magnesium, barium, calcium, aluminium, iron, cadmium, or strontium, in admixture with water. The oxide combines with phosphoric acid liberated during setting.…
A quick setting cement, particularly for use in dentistry, comprises a mono-metallic phosphate of a polyvalent metal of the third to the eleventh series which can form a water-insoluble tri-metallic phosphate by admixture with water, in admixture with an oxide and/or a silicate…
A quick setting cement comprises a dehydrated metal dihydrogen phosphate and a metal silicate having a metal oxide/silica ratio of at least one, where the metal is calcium, magnesium, barium, zinc, aluminium, iron, cadmium, or strontium, in admixture with water. Dehydration is…