A steel of high cleanliness is produced through satisfactory elimination of nonmetallic inclusions. There is disclosed a process for producing a high cleanliness steel, comprising the step of subjecting a molten steel outputted from a converter (1) to ladle refining and…
Kimura Sei
A useful process in which a steel material for obtaining a steel wire material reduced in the content of hard non-rollable inclusions and having enhanced drawability and enhanced fatigue characteristics is produced by adequately controlling conditions in secondary refining and…
The number of blades (16) of an impeller (10), as well as the relations between the height (b0) of the base of the blade (16) and the height (b1) of the tip end, between the width (d) of the blade (16) and the diameter or width of a hot meal channel, between the maximum depth…
A steel wire rod is obtained, in which a gas flow rate during gas stirring in molten steel treatment is controlled to be 0.0005 Nm 3 /min to 0.004 Nm 3 /min per molten steel of 1 ton, thereby the rod satisfies a specified composition, and oxide base inclusions in any section…
High cleanliness spring steel useful in manufacturing a spring with SiO 2 -based inclusions being extremely controlled and excellent in fatigue properties is provided. High cleanliness spring steel which is steel containing; C: 1.2% (means mass %, hereafter the same with respect…
A steel for high-cleanliness springs which is significantly reduced in the content of SiO2 inclusions and is useful for producing a spring having excellent fatigue characteristics. The steel for high-cleanliness springs is a steel which contains, in terms of mass%, 0-1.2%,…