Hard particles for blending as a starting material in a sintered alloy contain 20 to 40 mass % of molybdenum, 0.5 to 1.0 mass % of carbon, 5 to 30 mass % of nickel, 1 to 10 mass % of manganese, 1 to 10 mass % of chromium, 5 to 30 mass % of cobalt, 0.05 to 2 mass % of yttrium,…
Kikko Tadayoshi
There is provided an iron-based mixture powder for sintering, as well as an iron-based sintered alloy using same, that are capable of reducing the cutting resistance of the iron-based sintered alloy and of mitigating the shortening of cutting tool life even when a metal fluoride…
There is provided an iron-based mixture powder for sintering, as well as an iron-based sintered alloy using same, that are capable of reducing the cutting resistance of the iron-based sintered alloy and of mitigating the shortening of cutting tool life even when a metal fluoride…
Hard particles for blending as a starting material in a sintered alloy contain 20 to 40 mass% of molybdenum, 0.5 to 1.0 mass% of carbon, 5 to 30 mass% of nickel, 1 to 10 mass% of manganese, 1 to 10 mass% of chromium, 5 to 30 mass% of cobalt, 0.05 to 2 mass% of yttrium, and the…
There is provided an iron-based mixture powder for sintering, as well as an iron-based sintered alloy using same, that are capable of reducing the cutting resistance of the iron-based sintered alloy and of mitigating the shortening of cutting tool life even when a metal fluoride…