US 2007260016 A1#130060 Most Cited · 133 citations7.0/yr · PR 15.88PendingUS · Application
Linear low density polymer blends and articles made therefrom

This invention relates to blends of linear low density polyethylene copolymers with other linear low density polyethylenes or very low density, low density, medium density, high density, and differentiated polyethylenes. The invention also includes articles produced from the…

WO 0,198,409 A1#1060156 Most Cited · 47 citations1.9/yr · PR 4.68PendingWO · Application
Very low density polyethylene and high density polyethylene blends

Blends of very low density polyethylene produced using metallocene catalysts (mVLDPE) and high density polyethylene (HDPE) are disclosed. The polymer blends include a metallocene-catalyzed VLDPE polymer having a density of less than 0.916 g/cm3, the VLDPE polymer preferably…

US 2003213938 A1#1231592 Most Cited · 43 citations1.9/yr · PR 6.01PendingUS · Application
Metallocene-produced very low density polyethylenes

A very low density polyethylene having a density of 0.890 to 0.915 and a Dart Drop value of at least about 450 g/mil or above is disclosed. Gas phase polymerization methods are also disclosed for making very low density linear polyolefins utilizing a metallocene catalyst, and…

WO 2007/130277 A1#1379996 Most Cited · 40 citations2.1/yr · PR 8.86PendingWO · Application
Linear low density polymer blends and articles made therefrom

This invention relates to blends of linear low density polyethylene copolymers with other linear low density polyethylenes or very low density, low density, medium density, high density, and differentiated polyethylenes. The invention also includes articles produced from the…

US 2004014895 A1#4203065 Most Cited · 20 citations0.9/yr · PR 3.63PendingUS · Application
Very low density polyethylene and high density polyethylene blends

Blends of very low density polyethylene produced using metallocene catalysts (mVLDPE) and high density polyethylene (HDPE) are disclosed. The polymer blends include a metallocene-catalyzed VLDPE polymer having a density of less than 0.916 g/cm 3 , the VLDPE polymer preferably…

WO 2004/005357 A1#7747746 Most Cited · 13 citations0.6/yr · PR 2.09PendingWO · Application
Oxygen tailoring of polyethylene film resins

Processes are disclosed for oxygen-tailoring polyethylene resin. Polyethylene resin is conveyed through a feed zone, a melt-mixing zone and a melt zone. The resin is contacted with oxygen in an amount of at least 40 parts by weight O2 per million parts by weight resin, and…

WO 0,198,372 A2#8930145 Most Cited · 11 citations0.4/yr · PR 3.22PendingWO · Application
Metallocene-produced very low density polyethylenes

A very low density polyethylene having a density of 0.890 to 0.915 and a Dart Drop value of at least about 450 g/mil or above is disclosed. Gas phase polymerization methods are also disclosed for making very low density linear polyolefins utilizing a metallocene catalyst, and…

US 2004039131 A1#10652420 Most Cited · 10 citations0.5/yr · PR 1.86PendingUS · Application
Oxygen tailoring of polyethylene film resins

Processes are disclosed for oxygen-tailoring polyethylene resin. Polyethylene resin is conveyed through a feed zone, a melt-mixing zone and a melt zone. The resin is contacted with oxygen in an amount of at least 40 parts by weight O 2 per million parts by weight resin, and…

US 2006079664 A1#37617414 Most Cited · 2 citations0.1/yr · PR 1.10PendingUS · Application
Oxygen tailoring of polyethylene blow molding resins
Inventors: Poloso Anthony, Johnson Jerry MAssignee: Poloso Anthony, Johnson Jerry MFiled 2004-10-08

Processes are disclosed for oxygen-tailoring polyethylene blow molding resin. Polyethylene resin is conveyed through a feed zone, a melt-mixing zone and a melt zone, wherein the temperature of the polyethylene resin is from about 216° C. to about 260° C. in the melt zone. The…

WO 0,198,372 A3#63849573 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Metallocene-produced very low density polyethylenes

A very low density polyethylene having a density of 0.890 to 0.915 and a Dart Drop value of at least about 450 g/mil or above is disclosed. Gas phase polymerization methods are also disclosed for making very low density linear polyolefins utilizing a metallocene catalyst, and…

WO 2006/041605 A1#131813172 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Oxigen tailoring of polyethylene blow molding resins

Processes are disclosed for oxygen-tailoring polyethylene blow molding resin. Polyethylene resin is conveyed through a feed zone, a melt-mixing zone and a melt zone, wherein the temperature of the polyethylene resin is from about 216 °C to about 260 °C in the melt zone. The…