Reusable core carbon-carbon composite brake disc

Method of manufacturing carbon-carbon composite brake disc comprising a dense reusable core. Preferably, the reusable core has a density of 1.8-2.05 g/cc. The method includes: forming a dense carbon-carbon composite core; positioning the dense core in a location within a…

WO 2005/116476 A2#3729901 Most Cited · 22 citations1.1/yr · PR 2.91PendingWO · Application
Reusable core carbon-carbon composite brake disc

Method of manufacturing carbon-carbon composite brake disc (5, 17, 35) comprising a dense reusable core 7, 19, 37). Preferably, the reusable core has a density of 1 .8-2.05 g/cc. The method includes: forming a dense carbon-carbon composite core; positioning the dense core in a…

US 2007193836 A1#4340337 Most Cited · 20 citations1.1/yr · PR 2.14PendingUS · Application
Method and brake disc with composite insert member

A method and a brake disc with a composite insert member is disclosed. The method discloses the coupling of a carbon-carbon composite insert member with the brake disc to provide an interface for the brake disc.

US 2005271876 A1#10798458 Most Cited · 10 citations0.5/yr · PR 1.64PendingUS · Application
Method for producing carbon-carbon brake material with improved initial friction coefficient or 'bite'

Method of manufacturing a brake pad that has improved initial friction coefficient or “bite”. The method involves molding a carbon-carbon preform into the desired shape; carbonizing the preform by gradually heating it to 650-900° C. and holding it at that temperature for…

WO 2005/121592 A1#34057134 Most Cited · 3 citations0.1/yr · PR 0.96PendingWO · Application
Method for producing carbon-carbon brake material with improved initial friction coefficient or “bite”

Method of manufacturing a brake pad that has improved initial friction coefficient or “bite”. The method involves molding a carbon-carbon preform into the desired shape; carbonizing the preform by gradually heating it to 650-900°C and holding it at that temperature for…

WO 2005/116476 A3#99084481 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Reusable core carbon-carbon composite brake disc

Method of manufacturing carbon-carbon composite brake disc (5, 17, 35) comprising a dense reusable core 7, 19, 37). Preferably, the reusable core has a density of 1 .8-2.05 g/cc. The method includes: forming a dense carbon-carbon composite core; positioning the dense core in a…