A method to grain refine and deoxidize a precious metal alloy or a master alloy includes the steps of (a) forming a precursor melt consisting essentially of constituents of the precious metal alloy or master alloy and inevitable impurities; (b) dispersing a compound selected…
Assignee / Organization
Johns Peter G
28Total Forward Citations
9Indexed Patents
3Avg Citations / Patent
2Portfolio H-Index
An alkanethiol, alkyl thioglycollate, dialkyl sulfide or dialkyl disulfide may be used to surface treat of an alloy of silver containing an amount of germanium that is effective to reduce firestain and/or tarnishing. The treatment has been found to further reduce tarnishing of…
A firestain and tarnish-resistant ternary alloy of silver, copper and germanium contains from more than 93.5 wt % to 95.5 wt % Ag, from 0.5 to 3 wt % Ge and the remainder, apart from incidental ingredients (if any), impurities and grain refiner, copper. In order to further…