hottub.patents
WO 9,603,531 A1#4155575 Most Cited · 20 citations0.7/yr · PR 4.29PendingWO · Application
Aluminum alloys and process for making aluminum alloy sheet

An alloy of aluminum containing magnesium, silicon and optionally copper in amounts in percent by weight as shown in the figure, i.e. approximately falling within one of the following ranges: (1) 0.4 « Mg < 0.8, 0.2 « Si < 0.5, 0.3 « Cu « 3.5; (2) 0.8 « Mg « 1.4, 0.2 « Si…

WO 0,005,426 A1#6113600 Most Cited · 15 citations0.6/yr · PR 3.84PendingWO · Application
High conductivity aluminum fin alloy

An improved aluminum alloy fin stock is described having both a high strength and a high thermal conductivity. The fin stock contains 1.2 - 1.8 % Fe, 0.7 - 0.95 % Si, 0.3 - 0.5 % Mn, and the balance Al, and is produced by continuously strip casting the alloy at a cooling rate…

WO 0,153,553 A1#9013532 Most Cited · 11 citations0.4/yr · PR 2.88PendingWO · Application
Process of producing aluminum fin alloy

An aluminum alloy finstock of lower (more negative) corrosion potential and higher thermal conductivity than its elemental composition would normally provide is produced by a specific process. The process comprises continuously strip casting the alloy to form a strip, optionally…

WO 0,153,552 A1#11862338 Most Cited · 9 citations0.4/yr · PR 1.89PendingWO · Application
High thermal conductivity aluminum fin alloys

A method of producing an aluminum alloy finstock material, comprising the steps of continuously strip casting an aluminum finstock alloy to form an as-cast strip, rolling the as-cast strip to form a sheet article of intermediate gauge, annealing the sheet article of intermediate…

WO 9,923,269 A1#14985013 Most Cited · 7 citations0.3/yr · PR 1.89PendingWO · Application
Process for producing base foils of aluminum alloys

A process for the production of a base foil of an aluminum alloy is provided which comprises a first heating step in which a cold-rolled plate derived from a continuously cast-rolled plate is maintained at a temperature between higher than 350 °C and lower than 450 °C for longer…

WO 02,064,848 A1#21637892 Most Cited · 5 citations0.2/yr · PR 1.35PendingWO · Application
Production of high strength aluminum alloy foils

An aluminum alloy foil is formed from an alloy containing about 1.2 to 1.7% by weight iron, about 0.4 to 0.8% by weight silicon and about 0.07 to 0.20% by weight manganese, with the balance aluminum and incidental impurities. The alloy is continuously strip cast, e.g. on a belt…

WO 0,066,799 A1#29889214 Most Cited · 3 citations0.1/yr · PR 1.26PendingWO · Application
Production of aluminum alloy strip for use in making thin gauge foils

A continuous cast aluminum alloy strip is used in the production of thin gauge or converter foils. The alloy strip contains 0.4 to 0.8 % by weight Fe and 0.2 to 0.4 % by weight Si, has an as cast thickness of less than about 30mm and contains a substantially single intermetallic…

WO 9,906,606 A1#29978731 Most Cited · 3 citations0.1/yr · PR 1.26PendingWO · Application
Cast metal-matrix composite material and its use

A metal-matrix composite material includes a matrix having magnetsium in an amount of more than about 0.3 weight percent but no more than about 2.5 weight percent, an alloying element of about 0.8 to about 2.5 weight percent iron or from about 1.0 to about 2.5 weight percent…

CA 1,302,740 C#45027415 Most Cited · 2 citations0.1/yr · PR 0.88ExpiredCA · Utility
Aluminum alloys and a method of production
Inventors: Jin Iljoon, Lloyd David JAssignee: Jin IljoonFiled 1987-08-18 · Granted 1992-06-09

Abstract A new family of medium and high strength, thermally stable aluminum based alloys are described having the following composition: 0.4 to 1.2% by weight chromium, 0.3 to 0.8% by weight zirconium, 1.5 to 2.5% by weight manganese, 0 to 2.0% by weight magnesium and the…

WO 0,008,218 A1#48757848 Most Cited · 1 citations0.0/yr · PR 0.89PendingWO · Application
Preparation of metal-matrix composite materials with high particulate loadings by concentration

A composite material having less than about 25 volume percent refractory particles in a metal matrix is concentrated to have about 37-45 volume percent refractory particles. The concentrating is preferably accomplished by heating the composite material to melt the matrix, and…

WO 02,064,849 A1#47679835 Most Cited · 1 citations0.0/yr · PR 0.96PendingWO · Application
Production of aluminum alloy foils having high strength and good rollability

An aluminum alloy foil is formed from an alloy containing about 1.2 to 1.7 % by weight Fe and about 0.35 to 0.80 % by weight Si, with the balance aluminum and incidental impurities. The alloy is continuously strip cast to form a strip having a thickness less than about 25 mm,…

WO 2005/032744 A1#61298886 Most Cited · 1 citations0.1/yr · PR 0.75PendingWO · Application
Belt casting of non-ferrous and light metals and apparatus therefor

ABSTRACT A casting belt for using in a single-belt or twin-belt casting apparatus is disclosed. The casting belt is made of aluminum alloy such as an alloy from the AA5XXX and AA6XXX systems, preferably having a thickness in the range of 1 to 2 mm. The aluminum casting belt of…

WO 9,923,269 B1#102333530 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Process for producing base foils of aluminum alloys

A process for the production of a base foil of an aluminum alloy is provided which comprises a first heating step in which a cold-rolled plate derived from a continuously cast-rolled plate is maintained at a temperature between higher than 350 °C and lower than 450 °C for longer…