A method of waste treatment and a stable waste elemental composition, particularly for use with arsenic-containing waste. As 2 O 3 The waste is slurried with CaO in water for 6-24 hours to produce calcium arsenate (III). Excess CaO for As is used to consume other waste. Drying…
Assignee / Organization
James Hamilton Kyle
14Total Forward Citations
3Indexed Patents
5Avg Citations / Patent
1Portfolio H-Index
METHODS FOR WASTE TREATMENT AND COMPOSITIONS OF STABILIZED WASTE ELEMENTS ARE PROVIDED, TYPICALLY FOR THE DISPOSAL OF ARSENICAL WASTES. ARSENIC TRIOXIDE WASTE PRODUCED AS A BY-PRODUCT OF METAL EXTRACTION IS SLURRIED IN WATER FOR FROM 6 TO 24 HOURS WITH FINELY DIVIDED QUICKLIME…