A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
Iza Michael
A chemical vapor deposition reactor is provided which includes a process chamber accommodating a substrate holder for multiple substrates, and a reactor gas inlet which supplies the reactant gases to a portion above the surface of the heated substrates. The reactant gases can be…
A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
A method for fabricating a III-nitride semiconductor film, comprising depositing or growing a III-nitride semiconductor film in a semiconductor light absorbing or light emitting device structure; and growing a textured or structured surface of the III-nitride nitride…
A nitride light emitting diode, on a patterned substrate, comprising a nitride interlayer having at least two periods of alternating layers of InxGa1−xN and InyGa1−yN where 0<x<1 and 0≰y<1, and a nitride based active region having at least one quantum well structure on…
A nitride light emitting diode, on a patterned substrate, comprising a nitride interlayer having at least two periods of alternating layers of InxGa1_xN and InyGa1_yN where0 < x < 1 and 0 ≤ y < 1, and a nitride based active region having at least one quantum well…
A chemical vapor deposition reactor is provided which includes a process chamber accommodating a substrate holder for multiple substrates, and a reactor gas inlet which supplies the reactant gases to a portion above the surface of the heated substrates. The reactant gases can be…
A method for growing an improved quality device by depositing a low temperature (LT) magnesium (Mg) doped nitride semiconductor thin film. The low temperature Mg doped nitride semiconductor thin film may have a thickness greater than 50 nm. A multi quantum well (MQW) active…
A method for growing a semi-polar nitride semiconductor thin film via metalorganic chemical vapor deposition (MOCVD) on a substrate, wherein a nitride nucleation or buffer layer is grown on the substrate prior to the growth of the semi-polar nitride semiconductor thin film.
A method for enhancing growth of device-quality planar semipolar nitride semiconductor thin films via metalorganic chemical vapor deposition (MOCVD) by using an (Al,In,Ga)N nucleation layer containing at least some indium. Specifically, the method comprises loading a substrate…
A method for enhancing growth of device-quality planar semipolar nitride semiconductor thin films via metalorganic chemical vapor deposition (MOCVD) by using an (Al,In,Ga)N nucleation layer containing at least some indium. Specifically, the method comprises loading a substrate…
A chemical vapor deposition reactor is provided which includes a process chamber accommodating a substrate holder for multiple substrates, and a reactor gas inlet which supplies the reactant gases to a portion above the surface of the heated substrates. The reactant gases can be…
A chemical vapor deposition reactor is provided which includes a process chamber accommodating a substrate holder for multiple substrates, and a reactor gas inlet which supplies the reactant gases to a portion above the surface of the heated substrates. The reactant gases can be…
A nitride light emitting diode, on a patterned substrate, comprising a nitride interlayer having at least two periods of alternating layers of In x Ga 1-x N and In y Ga 1-y N where 0<x<1 and 0≦y<1, and a nitride based active region having at least one quantum well…
A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
A method for growing a semi-polar nitride semiconductor thin film via metalorganic chemical vapor deposition (MOCVD) on a substrate, wherein a nitride nucleation or buffer layer is grown on the substrate prior to the growth of the semi-polar nitride semiconductor thin film.
A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
A method of controlled p-type conductivity in (Al,In,Ga,B)N semiconductor crystals. Examples include {10 1 1} GaN films deposited on {100} MgAl 2 O 4 spinel substrate miscut in the <011> direction. Mg atoms may be intentionally incorporated in the growing semipolar nitride…
A method for growing a semi-polar nitride semiconductor thin film via metalorganic chemical vapor deposition (MOCVD) on a substrate, wherein a nitride nucleation or buffer layer is grown on the substrate prior to the growth of the semi-polar nitride semiconductor thin film.
A method for improving the growth morphology of (Ga,Al,In,B)N thin films on nonpolar or semipolar (Ga,Al,In,B)N substrates, wherein a (Ga,Al,In,B)N thin film is grown directly on a nonpolar or semipolar (Ga,Al,In,B)N substrate or template and a portion of the carrier gas used…
A method for improved growth of a semipolar (Al,In,Ga,B)N semiconductor thin film using an intentionally miscut substrate. Specifically, the method comprises intentionally miscutting a substrate, loading a substrate into a reactor, heating the substrate under a flow of nitrogen…
A method of controlled p-type conductivity in (Al, In, Ga, B)N semiconductor crystals. Examples include { 1011 } GaN films deposited on {100} MgAl2O4 spinel substrate miscut in the <011> direction. Mg atoms may be intentionally incorporated in the growing semipolar nitride…
A method for growing an improved quality device by depositing a low temperature (LT) magnesium (Mg) doped nitride semiconductor thin film. The low temperature Mg doped nitride semiconductor thin film may have a thickness greater than 50nm. A multi quantum well (MQW) active layer…
A method for enhancing growth of device-quality planar semipolar nitride semiconductor thin films via metalorganic chemical vapor deposition (MOCVD) by using an (Al,In,Ga)N nucleation layer containing at least some indium. Specifically, the method comprises loading a substrate…