A tricalcium-phosphate-based prosthetic material is disclosed, which is a sintered ceramic body mainly consisting of tricalcium phosphate containing a limited amount of zinc, which is a known element having an osteogenesis-promoting effect, in the form of a solid solution. By…
Ito Atsuo
A method of making bonded SOS substrate with a semiconductor film on or above a sapphire substrate by implanting ions from a surface of the semiconductor substrate to form an ion-implanted layer; activating at least a surface of one of the sapphire substrate and the…
It is intended to provide a porous calcium phosphate article with a high strength which has pores of 70 μm or above (preferably large pores of 100 μm or above) penetrating the porous article, a structure wherein these pores are arranged to form a three-dimensional network and a…
A method for minimizing thickness variation of a substrate in an anneal step and achieving the smoothing of the surface of the substrate. Specifically provided is a method for treating the surface of a SOI substrate, including the steps of treating the surface of the SOI…
A process for producing an SOI wafer with enhanced SOI layer thickness uniformity, in which the occurrence of thermal strain, peeling, cracking, etc. on transparent insulating substrate and SOI layer can be prevented through simple and easy processing. There is provided a…
PROBLEM TO BE SOLVED: To prepare a suspension or a particle-solvent mixed system containing zinc-containing calcium phosphate particles and a therapeutic agent for zinc deficiency disorders. SOLUTION: The suspension or particle-solvent mixed system is obtained by mixing…
When manufacturing a bonded substrate using an insulator substrate as a handle wafer, there is provided a method for manufacturing a bonded substrate which can be readily removed after carried and after mounted by roughening a back surface of the bonded substrate (corresponding…
A process for producing a laminated substrate which comprises: a step in which an oxide film is formed on a surface of a first substrate having a hardness of 150 GPa or higher in terms of Young's modulus and the oxide film is flattened; a step in which hydrogen ions,…
A porous calcium phosphate high molecular weight hydrogel composite having through holes which has artificial three-dimensional through holes having a diameter of 70 μm to 4 mm, has a porosity of 20 to 80 %, and contains calcium phosphate having a Ca/P mole ratio of 0.75 to 2.1…
The staining and sticking system is composed of a staining device and a sticking device, which is provided separately from the staining device, is capable of lightening the staining and sticking work and can be downsized. The staining and sticking system comprises the staining…
A plasma treatment or an ozone treatment is applied to the respective bonding surfaces of the single-crystal Si substrate in which the ion-implanted layer has been formed and the quartz substrate, and the substrates are bonded together. Then, a force of impact is applied to the…
On a surface side (bonding side) of a single crystal Si substrate (10), a uniform ion implantation layer (11) is formed at a prescribed depth (average ion implantation depth (L)) in the vicinity of the surface. The single crystal Si substrate (10) and a transparent insulating…
The problem of a defect density increase due to lattice constant mismatch between silicon and sapphire is solved, and an SOS substrate having a low defect density is provided. The bonded SOS substrate (8) has a semiconductor thin film (4) provided on the surface of a sapphire…
Provided is an organic material optical sheet for a condenser-type solar cell that displays excellent durability with respect to sunlight and can be easily worked into the shape of a Fresnel lens. Specifically, provided is an organic material optical sheet for a condenser-type…
A method for producing a single crystal silicon solar cell including the steps of: implanting ions into a single crystal silicon substrate through an ion implanting surface thereof to form an ion implanted layer in the single crystal silicon substrate; forming a transparent…
A bonded SOS substrate having a semiconductor film on or above a surface of a sapphire substrate is obtained by a method with the steps of implanting ions from a surface of a semiconductor substrate to form an ion-implanted layer; activating at least a surface from which the…
Hydrogen ions are implanted to a surface (main surface) of the single crystal Si substrate 10 at a dosage of 1.5×10 17 atoms/cm 2 or higher to form the hydrogen ion implanted layer (ion-implanted damage layer) 11 . As a result of the hydrogen ion implantation, the hydrogen ion…
A heating plate (32) having a smooth surface is placed on a hot plate (31) which constitutes a heating section, and the smooth surface of the heating plate (32) is adhered on the rear surface of a single crystal Si substrate (10) bonded to a transparent insulating substrate…
A staining and sticking system composed of a staining device and a sticking device provided separately from the staining device, enabling further lightening of the staining and sticking work, and having a small size. The staining and sticking system comprises a staining device…
A suspension or a particle-solvent mixture system, which contains microparticles of zinc-containing calcium phosphate with particular chemical composition, specifically, microparticles of sparingly soluble zinc-containing calcium phosphate, and a therapeutic agent for treating…
To provide a method of manufacturing a laminated wafer by which a strong coupling is achieved between wafers made of different materials having a large difference in thermal expansion coefficient without lowering a maximum heat treatment temperature as well as in which cracks or…
Provided is a method for manufacturing an SOI wafer, which is capable of: efficiently removing an ion-implanted defect layer existing in an ion implanted layer in the vicinity of a peeled surface peeled by an ion implantation peeling method; ensuring the in-plane uniformity of a…
The present invention relates to a solar cell module which is characterized in that: a light-transmitting elastomer member and a solar cell element are arranged in a space between a panel of a transparent member upon which sunlight is incident and a panel of a thermally…
Disclosed is a process for producing an SOI wafer that can efficiently remove an ion-implanted defect layer present in an ion-implanted layer near a flaked face flaked by an ion implantation flaking method, can ensure the in-plane evenness of a substrate, and can realize lowered…
PROBLEM TO BE SOLVED: To obtain a zinc sustained release ceramic which has high biocompatibility and is used for living bodies. SOLUTION: This zinc sustained release ceramic used for living bodies comprises tricalcium phosphate [Ca3(PO4)2] containing Zn in an amount of 0.0126 to…