Cooking vessel intended to be induction heated, comprising a heating part made of a ferromagnetic alloy having a Curie temperature of between 150° C. and 370° C. and a magnetostriction coefficient λ s ≦5×10 −6 in absolute value. FeNiCuX ferromagnetic alloy for the manufacture of…
Imphy Ugine Precision
An iron--cobalt alloy the chemical composition of which comprises, by weight: 35%≦Co≦55%; 0.5%≦V≦2.5%; 0.02%≦Ta+2×Nb≦0.2%; 0.0007%≦B≦0.007%; C≦0.05%; the balance being iron and impurities resulting from the smelting operation.
The invention concerns a treatment method which consists in coating at least one surface of a brittle thin metal strip ( 1 ) with a coating film ( 3, 3' ) comprising at least a polymer material, to obtain on the strip an adhering coat with a thickness ranging between 1 and…
A strip (1') of nanocrystalline material with a weak magnetic permeability wound on itself, is in the form of a toric reel (3) and is obtained from a ribbon (1) cast in an amorphous state, of an atomic composition: (Fe1-aMa)100-x-y-z- alpha - beta - psi CuxSiyBzNb alpha…
A device for masking a flat screen color monitor has a mask mounted within and tensioned at ambient temperature by a support. The support is an iron nickel alloy with a thermal expansion coefficient ≤ 5 x 10<-6>/K between 20 - 150 degrees C and an elastic limit Rp0.2 at 20…
The invention concerns an iron-cobalt alloy, characterised in that it comprises in weight percentages: 10 to 22% of Co; traces to 2.5% of Si; traces to 2% of Al; 0.1 to 1% of Mn; traces to 0.0100% of C; a total of O, N and S content ranging between traces and 0.0070%; a total of…
The invention concerns a treatment method which consists in coating at least one surface of a brittle thin metal strip ( 1 ) with a coating film ( 3, 3′ ) comprising at least a polymer material, to obtain on the strip an adhering coat with a thickness ranging between 1 and 100…
The invention concerns a method for making a strip or a workpiece cut out from a cold rolled maraging steel strip and hardened by a hardening heat treatment, which consists, prior to the heat treatment, in subjecting the strip or the workpiece to cold plastic deformation with a…
A maraging steel strip or part and process for manufacture of a strip or of a part cut out of a strip of cold-rolled maraging steel and hardened by a hardening heat treatment. In the process, before the hardening heat treatment is performed, the strip or the part is subjected to…
Soft magnetic alloy of the iron-nickel type, the chemical composition of which comprises, by weight: 40%≦Ni+Co≦65%; 0%≦Co≦7%; 2%≦Cr≦5%; 1%≦Ti≦3%; 0%≦Al≦0.5%; 0%≦Mn+Si≦2%; optionally, up to 3% Mo, 2% W, 2% V, 1.5% Nb, 1% Ta and 3% Cu, the sum of the Cr, Mo, W, V, Nb, Ta and Cu…
Soft magnetic alloy of the iron-nickel type, the chemical composition of which comprises, in % by weight: 34%<=Ni<=40%; 7%<=Cr<=10%; 0.5%<=Co<=3%; 0.1%<=Mn<=1%; O<=0.007%; S<=0.002%; N<=0.004%; with N+S+O<=0.01%; iron and impurities 5…
A maraging steel preferably without cobalt, having the following chemical composition: Ni 18-23 wt. %, Mo 4.5-8 wt. %, Ti 1-2 wt. %, Al 0-0.3 wt. %, C</=0.01 wt. %, remainder Fe and impurities. The composition also preferably satisfies the following conditions: Ni+Mo=23-27…
Process for manufacturing a strip made of an Fe—Ni alloy of the “γ′ and/or γ″ structural hardening” type, the thermal expansion coefficient between 20° C. and 150° C. of which is less than 7×10 −6 /K, in which a hot strip is manufactured either by hot rolling a semi-finished…
The container comprises a heating part made from a ferromagnetic alloy of the type FeNiCuX (X= Cr, Mo, Mn, Si, Al, W, Nb, V and Ti) having a Curie temperature of 150-370 degrees C, preferably below 350 degrees C, and a magnetostriction coefficient lambda s of at most 5 x…
A maraging steel strip or part and process for manufacture of a strip or of a part cut out of a strip of cold-rolled maraging steel and hardened by a hardening heat treatment. In the process, before the hardening heat treatment is performed, the strip or the part is subjected to…
The invention concerns a treatment method which consists in coating at least one surface of a brittle thin metal strip ( 1 ) with a coating film ( 3, 3 ′) comprising at least a polymer material, to obtain on the strip an adhering coat with a thickness ranging between 1 and 100…
The invention concerns an iron-cobalt alloy, characterised in that it comprises in weight percentages: 10 to 22% of Co; traces to 2.5% of Si; traces to 2% of Al; 0.1 to 1% of Mn; traces to 0.0100% of C; a total of O, N and S content ranging between traces and 0.0070%; a total of…
An iron-cobalt alloy the chemical composition of which comprises, by weight: 35%<=Co<=55%; 0.5%<=V<=2.5%; 0.02%<=Ta+2xNb<=0.2%; 0.0007%<=B<=0.007%; C<=0.05%; the balance being iron and impurities resulting from the smelting operation.
A method for the fabrication of Fe-Ni alloy strip consists of:- a) fabricating a hot rolled strip by hot rolling a semi-product, from direct thin strip casting and possibly light hot rolling, and subjecting it to tempering at a temperature between 950 and 1200 degrees C followed…
The invention relates to a soft magnetic alloy with the following composition in wt. %: 28%<= Ni <= 34%, 0% <= Co <= 4%, 0% <= Cu <= 4%, 1% <= Cr, 0% <= Mo <= 8 %, 0% <= Nb <= 1%, 0% <= Mn <= 2%, 0% <= V <= 5%, 0% <= W <= 5%, 0%…
A soft magnetic iron-nickel alloy, having a relatively low nickel content and containing chromium and cobalt, is new. A novel soft magnetic iron-nickel alloy has the composition (by wt.) 34-40% Ni, 7-10% Cr, 0.5-3% Co, 0.1-1% Mn, ≤ 0.007% ≤ 0.002% S, ≤ 0.004% N, balance Fe and…
Masking device for a color cathode-ray display tube with a flat scree, of the type comprising a support frame for a tensioned shadowmask and a tensioned shadowmask mounted on the support frame so as to undergo tensioning at room temperature, in which device the support frame is…
A shadow mask support frame for a cathode-ray color display tube of generally rectangular shape in top plan view. The shadow mask support frame includes two end upstands, which are located opposite each other and which are intended to support a shadow mask, and two lateral…
The invention concerns a method which consists in: cutting out in a metal sheet at least a planar plate (20) comprising a main part having the developed shape of the wall of the structural element and at least a matching overlapping and fixing part (26, 27, 28), folding the cut…
The invention concerns a method for making a strip or a workpiece cut out from a cold rolled maraging steel strip and hardened by a hardening heat treatment, which consists, prior to the heat treatment, in subjecting the strip or the workpiece to cold plastic deformation with a…