A method of manufacturing a porous body using particulate material as a starting stock. The particles are inserted in a can, the can evacuated and inert gas admitted to a predetermined back-fill pressure. After hot isostatic pressing, the compact so formed is cooled and…
Imi Titanium Ltd
Processes for manufacturing high T c superconductors by electrophoretic deposition onto a substrate or by coating onto the substrate a plurality of components in solution or suspension and subsequent heat treatment. The substrate is preferably conducting and may be silver and…
Creep resistant titanium alloys containing : Al---5,0 - 7,0 % Zr---2,0 - 7,0 % Mo 0,1 - 2,5 % Ge---0,01 - 10,0 % and optionally one or more of the following elements: Sn 2,0 - 6,0 % Nb 0,1 - 2,0 % C 0,02 - 0,1 % Si 0,1 - 2,0 %
A high strength titanium alloy capable of being used at elevated temperatures, the alloy containing 3.5-5.65% aluminium, 3.0-8.1% tin, with a total aluminium equivalent in the range 6.1-6.8%, 4.5-7.5% zirconium, 1.5-3% molybdenum, 0.2-0.6% silicon, balance titanium apart from…
A rotating or moving metal component such as a blade for a gas turbine engine is made from a composite bar of titanium alloy (10, 20, 40) with the sides of the bar having a surface layer (11, 21, 41) of eg. nickel which is less likely to ignite in particle form when present in…
A method of manufacturing a porous body using particulate material as a starting stock. The particles are inserted in a can, the can evacuated and inert gas admitted to a predetermined back-fill pressure. After hot isostatic pressing, the compact so formed is cooled and…
A weldable titanium alloy particularly intended for use at high temperatures and under conditions of high stress in aircraft engines, the alloy having the composition 5.6% aluminium, 4% tin, 4% zirconium, 1% niobium, 0.25% molybdenum, 0.5% silicon, 0.05% carbon, optionally…
Creep resistant titanium alloys containing aluminum, zirconium, molybdenum and germanium plus optional silicon, carbon, tin and niobium.
A method of producing a profiled plate in a metal alloy by rolling the plate through a four high mill, the work rolls having pockets to accommodate the thicker portion of the plate, the work rolls rolling the plate and discharging it on the side opposite the side into which it…
A weldable titanium alloy particularly intended for use at high temperatures and under conditions of high stress in aircraft engines, the alloy having the composition 5.6% aluminium, 4%tin, 4% zirconium, 1 %niobium, 0.25% molybdenum, 0.5% silicon, 0.05% carbon, optionally…
A high strength titanium alloy capable of being used at elevated temperatures, the alloy containing 3.5-5.65% aluminium, 3.0-8.1% tin, with a total aluminium equivalent in the range 6.1-6.8%, 4.5-7.5% zirconium, 1.5-3% molybdenum, 0.2-0.6% silicon, balance titanium apart from…
A method of producing a profiled plate in a metal alloy by rolling the plate (17) through a four high mill, the work rolls (3, 4) having pockets (13,14) to accommodate the thicker portion of the plate, the work rolls rolling the plate and discharging it on the side opposite the…
Abstract Titanium alloy A weldable titanium alloy particularly intended for use at high temperatures and under conditions of high stress in aircraft engines, the alloy having the composition 5.6% aluminum, 4% tin, 4% zirconium, 1% niobium, 0.25% molybdenum, 0.5% silicon, 0.05%…
ABSTRACT: A high strength titanium alloy capable of being used at elevated temperatures, the alloy containing 3.5-5.65% aluminium, 3.0-8.1% tin, with a total aluminium equivalent in the range 6.1-6.8%, 4.5-7.5% zirconium, 1.5-3% molybdenum, 0.2-0.6% silicon, balance titanium…
ABSTRACT A method of producing a profiled plate in a metal alloy by rolling the plate through a four high mill, the work rolls having pockets to accom-modate the thicker portion of the plate, the work rolls rolling the plate and discharging it on the side opposite the side into…
MnO2 is mfd. by electrolysis of a soln. contg. Mn ions, where an anode and cathode are placed in the soln. and a current passed between them to deposit MnO2 on the anode. The anode includes a hanger bar and a perpendicular dependent sheet of valve metal directly or indirectly…
In the manufacture of superconducting wires, tin-cored niobium sleeves are inserted in a drilled copper billet. The billet is then pre-cooled and extruded, and subsequently drawn down, and then heated to react the niobium and tin. The pre-cooling is sufficient to prevent the tin…