A steel for cold forging/nitriding, which contains 0.01-0.15% of C, 0.35% or less of Si, 0.10-0.90% of Mn, 0.030% or less of P, 0.030% or less of S, 0.50-2.0% of Cr, 0.10-0.50% of V, 0.01-0.10% of Al, 0.0080% or less of N and 0.0030% or less of O, and optionally contains a…
Imataka Hideki
Provided is a rolled steel bar or wire for hot forging, having excellent bending fatigue strength, surface fatigue strength, abrasion resistance, and machinability even after hot forging. This rolled steel bar or wire for hot forging has a chemical composition containing C, Si,…
A steel for cold forging/nitriding has, by mass percent, C: 0.01 to 0.15%, Si≦0.35%, Mn: 0.10 to 0.90%, P≦0.030%, S≦0.030%, Cr: 0.50 to 2.0%, V: 0.10 to 0.50%, Al: 0.01 to 0.10%, N≦0.0080%, and O≦0.0030%, further according to need a specific amount of one or more elements…
A rolled steel bar or wire for hot forging capable of achieving at a high level both bending/surface-fatigue strength and machinability of components is provided. The rolled steel bar or wire for hot forging comprises, in % by mass, 0.1-0.25% C, 0.01-0.10% Si, 0.4-1.0% Mn,…
A steel for nitriding having a chemical composition consisting of, by mass percent, C: 0.07-0.14%, Si: 0.10-0.30%, Mn: 0.4-1.0%, S: 0.005-0.030%, Cr: 1.0-1.5%, Mo: ≦0.05% (including 0%), Al: 0.010% or more to less than 0.10%, V: 0.10-0.25%, optionally at least one element…
A rolled steel bar or wire rod having hot surface fatigue strength, wear resistance, and machinability even after hot forging has a composition containing C, Si, Mn, S, Cr, Mo (optional), Al, and N, with the balance being Fe and impurities. The chemical composition satisfies…
Steel for nitriding, which has a chemical composition that contains 0.07-0.14% of C, 0.10-0.30% of Si, 0.4-1.0% of Mn, 0.005-0.030% of S, 1.0-1.5% of Cr, 0.05% of less of Mo (including 0%), 0.010% or more but less than 0.10% of Al and 0.10-0.25% of V, and if necessary 0.30% of…
A hot forged non-heat treated steel for induction hardening, comprising by mass percent, C: 0.35 to 0.45%, Si: 0.20 to 0.60%, Mn: 0.40 to 0.80%, S: 0.040 to 0.070%, Cr: 0.10 to 0.40%, Ti: 0.020 to 0.100%, Ca: 0.0005 to 0.0050%, B: 0.0005 to 0.0030%, 0: 0.0015 to 0.0050%, Mo: 0…
A rolled steel bar or a wire rod for hot forging capable of coping with both bending/surface fatigue strength of components and machinability at a high level includes: a composition containing, in mass %, C: 0.1 to 0.25%, Si: 0.01 to 0.10%, Mn: 0.4 to 1.0%, S: 0.003 to 0.05%,…
A steel for cold forging/nitriding has, by mass percent, C: 0.01 to 0.15%, Si≤0.35%, Mn: 0.10 to 0.90%, P≤0.030%, S≤0.030%, Cr: 0.50 to 2.0%, V: 0.10 to 0.50%, Al: 0.01 to 0.10%, N≤0.0080%, and O≤0.0030%, further according to need a specific amount of one or more elements…
A hot forged non-heat treated steel for induction hardening, which has a chemical composition that C: 0.35 to 0.45 %, Si: 0.20 to 0.60 %, Mn: 0.40 to 0.80 %, S:0.040 to 0.070 %, Cr: 0.10 to 0.40 %, Ti: 0.020 to 0.100 %, Ca: 0.0005 to 0.0050 %, B: 0.0005 to 0.0030 %, O: 0.0015 to…
A rolled steel bar or a wire rod for hot forging capable of coping with both bending/surface fatigue strength of components and machinability at a high level includes: a composition containing, in mass %, C: 0.1 to 0.25%, Si: 0.01 to 0.10%, Mn: 0.4 to 1.0%, S: 0.003 to 0.05%,…