Patents
US 2012129690 A1#1779451 Most Cited · 35 citations2.5/yr · PR 4.00PendingUS · Application
Porous inorganic composite oxide

A porous inorganic composite oxide containing oxides of aluminum and of cerium and/or zirconium, and, optionally, oxides of one or more dopants selected from transition metals, rare earths, and mixtures thereof, and having a specific surface area, in m 2 /g, after calcining at…

US 2013142713 A1#3487194 Most Cited · 23 citations1.8/yr · PR 3.02PendingUS · Application
Composition containing oxides of zirconium, cerium and at least one other rare earth and having a specific porosity, method for preparing same and use thereof in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2011-05-02

A composition is described that includes zirconium oxide, cerium oxide and yttrium oxide, or zirconium oxide, cerium oxide and at least two oxides of two rare earths different from cerium in a mass proportion of at least 20% of zirconium oxide and of at most 70% of cerium oxide,…

WO 2011/138255 A2#4248954 Most Cited · 20 citations1.3/yr · PR 3.17PendingWO · Application
Composition containing oxides of zirconium, cerium and at least one other rare earth and having a specific porosity, method for preparing same and use thereof in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Rhodia Operations, Ifrah SimonFiled 2011-05-02

The invention relates to a composition that contains zirconium oxide, cerium oxide and yttrium oxide, or zirconium oxide, cerium oxide and at least two oxides of two rare earths different from cerium in a mass proportion of at least 20 % of zirconium oxide and of at most 70 % of…

US 8,956,994 B2#5059245 Most Cited · 18 citations1.6/yr · PR 1.91ActiveUS · Utility
Composition containing oxides of zirconium, cerium and at least one other rare earth and having a specific porosity, method for preparing same and use thereof in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2011-05-02 · Granted 2015-02-17

A composition is described that includes zirconium oxide, cerium oxide and yttrium oxide, or zirconium oxide, cerium oxide and at least two oxides of two rare earths different from cerium in a mass proportion of at least 20% of zirconium oxide and of at most 70% of cerium oxide,…

US 2012046163 A1#5315725 Most Cited · 17 citations1.2/yr · PR 3.02PendingUS · Application
Composition including a lanthanum perovskite on an alumina or aluminium oxyhydroxide substrate, preparation method and use in catalysis

A composition is described that includes a perovskite of the formula LaMO 3 , where M is at least one element selected from among iron, aluminium or manganese, in the form of particles dispersed on an alumina or aluminium oxyhydroxide substrate, wherein after calcination at 700°…

US 2013052108 A1#7037016 Most Cited · 14 citations1.1/yr · PR 2.18PendingUS · Application
Composition containing oxides of zirconium, cerium and another rare earth having reduced maximum reducibility temperature, a process for preparation and use thereof in the field of catalysis

A composition is described that includes oxides of zirconium, cerium and another rare earth different from cerium, having a cerium oxide content not exceeding 50 wt % and, after calcination at 1000° C. for 6 hours, a maximal reducibility temperature not exceeding 500° C. and a…

US 2014205522 A1#10575221 Most Cited · 10 citations0.8/yr · PR 1.95PendingUS · Application
Composition based on oxides of cerium, of zirconium and of another rare earth metal with high reducibility, preparation process and use in the field of catalysis

The composition of the invention is based on oxides of cerium, of zirconium and of at least one rare earth metal other than cerium, with a cerium oxide content of greater than 50% by weight and it has, after calcination at 1000° C. for 4 hours, a specific surface area of at…

WO 2011/083157 A1#15927489 Most Cited · 7 citations0.5/yr · PR 1.47PendingWO · Application
Composition containing oxides of zirconium, cerium and another rare earth having reduced maximal reducibility temperature, and method for preparing and using same in the field of catalysis

The invention relates to a composition containing oxides of zirconium, cerium and another rare earth different from cerium, having a cerium oxide content not exceeding 50 wt% and, after calcination at 1000°C for 6 hours, a maximal reducibility temperature not exceeding 500°C and…

WO 2012/171947 A1#14914276 Most Cited · 7 citations0.5/yr · PR 1.94PendingWO · Application
Composition based on oxides of cerium, of zirconium and of another rare earth metal with high reducibility, preparation process and use in the field of catalysis

The composition of the invention is based on oxides of cerium, of zirconium and of at least one rare earth metal other than cerium, with a cerium oxide content of greater than 50% by weight and it has, after calcination at 1000°C for 4 hours, a specific surface area of at least…

US 2014044628 A1#18792521 Most Cited · 6 citations0.5/yr · PR 1.27PendingUS · Application
Composition based on oxides of zirconium, of cerium, of at least one rare earth other than cerium and of silicon, preparation processes and use in catalysis
Inventors: Ifrah SimonAssignee: Ifrah Simon, Rhodia OperationsFiled 2012-04-04

The composition according to the invention is based on zirconium oxide, cerium oxide and at least one oxide of a rare earth other than cerium, in a proportion, by weight, of zirconium oxide of at least 5% and of cerium oxide of at most 90%, and it is characterized in that it…

US 2014072492 A1#17267899 Most Cited · 6 citations0.5/yr · PR 1.78PendingUS · Application
Composition based on zirconium oxide and on at least one oxide of a rare earth other than cerium, having a specific porosity, processes for preparing same and use thereof in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2011-11-21

A composition of zirconium oxide and at least one oxide of a rare earth other than cerium is described. The zirconium oxide has a weight proportion of at least 50% and, after calcination at a temperature of 900° C. for 4 hours, the composition exhibits two populations of pores…

US 2012189517 A1#22310957 Most Cited · 5 citations0.4/yr · PR 1.18PendingUS · Application
Composition comprising cerium oxide and zirconium oxide having a specific porosity, preparation method thereof and use of same in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2010-07-02

A composition including cerium and zirconium oxides, including at least 30 wt.-% cerium oxide is desired. Following calcination at a temperature of 900 DEG C. for 4 hours, the composition has two populations of pores, the diameters of the first population being centered around a…

US 2014140910 A1#22279423 Most Cited · 5 citations0.4/yr · PR 1.20PendingUS · Application
Composition consisting of a ceria-zirconia mixed oxide with increased reducibility, production method and use in the field of catalysis

The invention relates to a composition essentially consisting of ceria-zirconia mixed oxide, with a ceria content of at least 60 wt. % and, after 4 hours of calcination at 1000° C., a specific surface area of at least 15 m 2 /g and a quantity of mobile oxygen between 200° C. and…

WO 2009/112356 A1#21632800 Most Cited · 5 citations0.3/yr · PR 1.35PendingWO · Application
Composition based on a zirconium oxide, a titanium oxide or a mixed zirconium titanium oxide on an alumina or aluminium oxyhydroxide support, methods of preparation and use as catalyst

The composition of the invention comprises at least one supported oxide chosen from zirconium oxide, titanium oxide or a mixed zirconium titanium oxide on an alumina-based or aluminium-oxyhydroxide-based support and is characterized in that, after calcination for 4 hours at…

WO 2010/100067 A1#20116444 Most Cited · 5 citations0.3/yr · PR 1.68PendingWO · Application
Composition including a lanthanum perovskite on an alumina or aluminium oxyhydroxide substrate, preparation method and use in catalysis

The composition according to the invention includes a perovskite of the formula LaMO 3 , where M is at least one element selected from among iron, aluminium or manganese, in the form of particles dispersed on an alumina or aluminium oxyhydroxide substrate, characterised in that…

US 8,974,764 B2#27122077 Most Cited · 4 citations0.4/yr · PR 1.10ActiveUS · Utility
Composition including a lanthanum perovskite on an alumina or aluminium oxyhydroxide substrate, preparation method and use in catalysis

A composition is described that includes a perovskite of the formula LaMO 3 , where M is at least one element selected from among iron, aluminum or manganese, in the form of particles dispersed on an alumina or aluminum oxyhydroxide substrate, wherein after calcination at 700°…

US 9,592,498 B2#27031901 Most Cited · 4 citations0.4/yr · PR 1.12ActiveUS · Utility
Porous inorganic composite oxide
Inventors: Larcher Olivier, Francis Francis, English Thomas, Ifrah Simon, Polli AndrewAssignee: Larcher Olivier, Francis FrancisFiled 2011-11-16 · Granted 2017-03-14

A porous inorganic composite oxide containing oxides of aluminum and of cerium and/or zirconium, and, optionally, oxides of one or more dopants selected from transition metals, rare earths, and mixtures thereof, and having a specific surface area, in m 2 /g, after calcining at…

WO 2011/006780 A1#25285367 Most Cited · 4 citations0.3/yr · PR 1.32PendingWO · Application
Composition comprising cerium oxide and zirconium oxide having a specific porosity, preparation method thereof and use of same in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Rhodia Operations, Ifrah SimonFiled 2010-07-02

The invention relates to a composition comprising cerium and zirconium oxides, containing at least 30 wt.-% cerium oxide. Following calcination at a temperature of 900°C for 4 hours, the composition has two populations of pores, the diameters of the first population being…

US 10,384,954 B2#33853080 Most Cited · 3 citations0.4/yr · PR 0.99ActiveUS · Utility
Composition comprising cerium oxide and zirconium oxide having a specific porosity, preparation method thereof and use of same in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2010-07-02 · Granted 2019-08-20

A composition including cerium and zirconium oxides, including at least 30 wt.-% cerium oxide is desired. Following calcination at a temperature of 900 DEG C. for 4 hours, the composition has two populations of pores, the diameters of the first population being centered around a…

US 8,524,183 B2#34040589 Most Cited · 3 citations0.2/yr · PR 0.96ActiveUS · Utility
Composition containing oxides of zirconium, cerium and another rare earth having reduced maximum reducibility temperature, a process for preparation and use thereof in the field of catalysis
Inventors: Ifrah Simon, Rohart Emmanuel, Hernandez Julien, Denaire StephaneAssignee: Ifrah Simon, Rohart EmmanuelFiled 2011-01-10 · Granted 2013-09-03

A composition is described that includes oxides of zirconium, cerium and another rare earth different from cerium, having a cerium oxide content not exceeding 50 wt % and, after calcination at 1000° C. for 6 hours, a maximal reducibility temperature not exceeding 500° C. and a…

WO 2013/004533 A1#32752818 Most Cited · 3 citations0.2/yr · PR 1.08PendingWO · Application
Composition consisting of a ceria-zirconia mixed oxide with increased reducibility, production method and use in the field of catalysis

The invention relates to a composition essentially consisting of a ceria-zirconia mixed oxide, with a ceria content of at least 60 wt. % and, after 4 hours of calcination at 1000°C, a specific surface area of at least 15 m 2 /g and a quantity of mobile oxygen between 200°C and…

WO 2013/004534 A1#31952980 Most Cited · 3 citations0.2/yr · PR 1.13PendingWO · Application
Composition consisting of a zirconia-ceria mixed oxide with increased reducibility, production method and use in the field of catalysis

The invention relates to a composition essentially consisting of a zirconia-ceria mixed oxide, with a zirconia content of at least 40 wt. % and, after 4 hours of calcination at 1000°C, a specific surface area of at least 25 m 2 /g and a quantity of mobile oxygen between 200°C…

US 10,189,010 B2#40133540 Most Cited · 2 citations0.3/yr · PR 1.01ActiveUS · Utility
Composition based on zirconium oxide and on at least one oxide of a rare earth other than cerium, having a specific porosity, processes for preparing same and use thereof in catalysis
Inventors: Ifrah Simon, Larcher OlivierAssignee: Ifrah Simon, Larcher OlivierFiled 2011-11-21 · Granted 2019-01-29

A composition of zirconium oxide and at least one oxide of a rare earth other than cerium is described. The zirconium oxide has a weight proportion of at least 50% and, after calcination at a temperature of 900° C. for 4 hours, the composition exhibits two populations of pores…

US 2014147357 A1#43839556 Most Cited · 2 citations0.2/yr · PR 0.92PendingUS · Application
Composition consisting of a zirconia-ceria mixed oxide with increased reducibility, production method and use in the field of catalysis

The invention relates to a composition essentially consisting of a zirconia-ceria mixed oxide, with a zirconia content of at least 40 wt. % and, after 4 hours of calcination at 1000° C., a specific surface area of at least 25 m 2 /g and a quantity of mobile oxygen between 200°…

US 8,563,462 B2#45241196 Most Cited · 2 citations0.1/yr · PR 0.87ActiveUS · Utility
Catalyst compositions based on nanoparticles of a zirconium oxide, a titanium oxide or a mixed zirconium/titanium oxide deposited onto a silica support therefor

Catalyst compositions include finely divided nanoscale particles of at least one supported oxide, based on a zirconium oxide, a titanium oxide or a mixed zirconium/titanium oxide deposited onto a silica based support, wherein, after calcination for 4 hours at 900° C., the…