The invention relates to a polycrystalline silicon rod that is characterised in that it has a rod cross-section having a surface ratio of between 50 - 99 % of silicon for electric conduction and the rod has a bending strength of between 0.1 to 80 N/mm2.
Hertlein Harald
The invention relates to a method for producing granulated polycrystalline silicon in a hot surface and fluidised bad reactor consisting in deposing a reaction gas containing a gaseous silicon compound in the form of a silicon metal on silicon particles, which are fluidised into…
Brittle polysilicon rods having a rod cross-section of 80-99% available for electrical conduction and a flexural strength of 0.1 to 80 N/mm 2 are produced by a process wherein the temperature of the bridge of polysilicon rods in the Siemens process is held at a high temperature…
High-purity polysilicon granules are prepared by depositing reaction gas on silicon granules in a fluidized bed reactor having: a reactor space comprising at least two zones lying one above the other, the lower zone weakly fluidized by introduction of a silicon-free gas into…
The invention relates to a method for producing granulated polycrystalline silicon in a hot surface and fluidised bad reactor consisting in deposing a reaction gas containing a gaseous silicon compound in the form of a silicon metal on silicon particles, which are fluidised into…
The invention relates to a polycrystalline silicon rod that is characterised in that it has a rod cross-section having a surface ratio of between 50 - 99 % of silicon for electric conduction and the rod has a bending strength of between 0.1 to 80 N/mm 2 .