Patents
Assignee / Organization

Heritier Philippe

48Total Forward Citations
11Indexed Patents
4Avg Citations / Patent
4Portfolio H-Index
WO 2006/114499 A2#6730783 Most Cited · 14 citations0.7/yr · PR 3.30PendingWO · Application
Tempered martensitic steel, method of producing a part from said steel and part thus obtained

The invention relates to steel which is characterised by the following composition as expressed in percentages by weight: - C = 0.18 0.30 %, - Co = 5 -7 %, - Cr = 2 - 5 %, - Al = 1 - 2 %, - Mo + W/2 = 1 - 4 %, - V = trace 0.3 %, - Nb = trace 0.1 %, - B = trace - 50 ppm, - Ni =…

US 2012183432 A1#8282453 Most Cited · 12 citations0.9/yr · PR 2.58PendingUS · Application
Nickel-based superalloy and parts made from said superalloy

A nickel superalloy has the following composition, the concentrations of the different elements being expressed as wt-%: Formula (I), the remainder consisting of nickel and impurities resulting from the production of the superalloy. In addition, the composition satisfies the…

WO 2011/020976 A1#14825923 Most Cited · 7 citations0.5/yr · PR 1.99PendingWO · Application
Nickel superalloy and parts made from said superalloy

The invention relates to a nickel superalloy having the following composition, the concentrations of the different elements being expressed as wt-%: Formula (I), the remainder consisting of nickel and impurities resulting from the production of said superalloy. In addition, the…

US 8,153,056 B2#22447427 Most Cited · 5 citations0.4/yr · PR 1.11ActiveUS · Utility
Hardened martensitic steel, method for producing a component from this steel and component obtained in this manner
Inventors: Montagnon Jacques, Heritier Philippe, Peslerbe Isabelle, Mons ClaudeAssignee: Montagnon Jacques, Heritier PhilippeFiled 2006-04-20 · Granted 2012-04-10

The invention relates to steel which is characterized by the following composition as expressed in percentages by weight:—C=0.18 0.30%, —Co=5-7%, —Cr=2-5%, —Al=1-2%, —Mo+W/2=1-4%, —V=trace 0.3%, —Nb=trace 0.1%, —B=trace−50 ppm, —Ni=10.5-15% with Ni≧7+3.5 Al, —Si=trace 0.4%,…

US 2012132326 A1#33607007 Most Cited · 3 citations0.2/yr · PR 1.02PendingUS · Application
Method for producing martensitic steel with mixed hardening

A method of producing a martensitic steel including a content of other metals such that it can be hardened by intermetallic compound and carbide precipitation, with an Al content of between 0.4% and 3%. The heat shaping temperature of a last heat shaping pass of the steel is…

US 8,152,938 B2#33957273 Most Cited · 3 citations0.2/yr · PR 0.98ActiveUS · Utility
Hardened martensitic steel, method for producing a component from this steel and component obtained in this manner
Inventors: Montagnon Jacques, Heritier Philippe, Peslerbe Isabelle, Mons ClaudeAssignee: Montagnon Jacques, Heritier PhilippeFiled 2010-08-26 · Granted 2012-04-10

The invention relates to steel which is characterized by the following composition as expressed in percentages by weight: —C=0.18 0.30%, —Co=5-7%, —Cr=2-5%, —Al=1-2%, —Mo+W/2=1-4%, —V=trace 0.3%, —Nb=trace 0.1%, —B=trace—50 ppm, —Ni=10.5-15% with Ni≧7+3.5 Al, —Si=trace 0.4%,…

US 8,192,560 B2#33957271 Most Cited · 3 citations0.2/yr · PR 0.98ActiveUS · Utility
Hardened martensitic steel, method for producing a component from this steel and component obtained in this manner
Inventors: Montagnon Jacques, Heritier Philippe, Peslerbe Isabelle, Mons ClaudeAssignee: Montagnon Jacques, Heritier PhilippeFiled 2010-08-26 · Granted 2012-06-05

The invention relates to steel which is characterized by the following composition as expressed in percentages by weight: —C=0.18 0.30%, —Co=5-7%, —Cr=2-5%, —Al=1-2%, —Mo+W/2=1-4%, —V=trace 0.3%, —Nb=trace 0.1%, —B=trace−50 ppm, —Ni=10.5-15% with Ni≧7+3.5 Al, —Si=trace 0.4%,…

WO 2011/001124 A1#62099129 Most Cited · 1 citations0.1/yr · PR 0.74PendingWO · Application
Method for producing martensitic steel with mixed hardening
Inventors: Ferrer Laurent, Heritier PhilippeAssignee: Snecma, Aubert & Duval SaFiled 2010-07-02

The invention relates to a method for producing martensitic steel that comprises a content of other metals such that the steel can be hardened by an intermetallic compound and carbide precipitation, with an Al content of between 0.4% and 3%. The heat shaping temperature for the…

US 8,702,879 B2#88367497 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for producing martensitic steel with mixed hardening
Inventors: Ferrer Laurent, Heritier PhilippeAssignee: Ferrer Laurent, Heritier PhilippeFiled 2010-07-02 · Granted 2014-04-22

A method of producing a martensitic steel including a content of other metals such that it can be hardened by intermetallic compound and carbide precipitation, with an Al content of between 0.4% and 3%. The heat shaping temperature of a last heat shaping pass of the steel is…

WO 2006/114499 A3#139657289 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Tempered martensitic steel, method of producing a part from said steel and part thus obtained

The invention relates to steel which is characterised by the following composition as expressed in percentages by weight: - C = 0.18 0.30 %, - Co = 5 -7 %, - Cr = 2 - 5 %, - Al = 1 - 2 %, - Mo + W/2 = 1 - 4 %, - V = trace 0.3 %, - Nb = trace 0.1 %, - B = trace - 50 ppm, - Ni =…

WO 2010/072972 A1#130733180 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for thermally processing a titanium alloy, and resulting part

The invention relates to a method for thermally processing a Ti 5-5-5-3 titanium alloy having the following composition in wt %: - between 4.4 and 5.7% of aluminium, - between 4.0 and 5.5% of vanadium, - between 0.30 and 0.50% of iron, - between 4.0 and 5.5% of molybdenum, -…