A nickel base alloy consists of:-Al : 1.0-9.0 per cent, Cr: 13.0 to 27.0 per cent, Co: over 10 but not over 35 per cent, Ti: 0.01 to 5.0 per cent, Si: 0 to 2.0 per cent, C: 0 to 1.5 per cent, N: 0 to 0.5 per cent, Fe and/or Mn: 0 to 3.0 per cent, Mo and/or W: 0 to 8.0 per cent,…
Harold Ernest Gresham
Nickel-base alloys which are strong and resistant to corrosion at high temperatures have the following ranges of compositions:-Aluminium 2-14 per cent., chromium 1-23 per cent., cobalt 0.1-10 per cent., nickel the remainder. The total of aluminium and chromium must be between 10…
519,902. Alloys: HALL, H. C., and GRESHAM, H. E. Oct. 7, 1938, No. 29085. [Classes 72 and 82 (i)] A copper alloy suitable for the sleeves of sleeve valves and for other parts of internal combustion engines contains 8-10.5 per cent. of aluminium, 0.25-0.6 per cent. of silicon,…
Sea-water valves, valves for internal combustion or steam engines, and other ferrous alloy parts which are subject to corrosion, are coated first by pressure, fusion or any other convenient method with a non-ferrous alloy having a melting point above 1100 DEG C., and then by…
489,384. Valves. GRESHAM, H. E. Feb. 3, 1937, Nos. 3181 and 19860. [Class 7(vi)] In poppet valves formed with a hollow stem to receive a coolant, the head is made in two parts welded together, either the outer or the inner part being integral with the stem, and the outer or both…
In a heat treatment process for light metals or alloys wherein a protective coating is provided on the article to be treated, the protective coating is sealed prior to heat treating. The sealing operation may be performed on an article of aluminium or aluminium alloy having an…
An article of aluminium base alloy is formed from an alloy having the following composition:-Mg 1 to 3.5 per cent, Ag 0.20 to 2.0 per cent, Mn 0.5 to less than 1 per cent, Al the remainder, and solutio-treated at 450 DEG to 550 DEG C. for 1 to 20 hours, quenched and aged at 120…
Porous metals, e.g. aluminium and aluminium alloys, are proofed against liquid, particularly glycol, by first subjecting to an anodic oxidation process and thereafter coating with a synthetic resin varnish of the thermo-hardening type and hardening by heating at gradually…
559,233. Deaerating oil &c. GRESHAM, H. E., and HEYWOOD, R. B. March 5, 1943, No. 4916/42. [Glass 1 (i)] [Also in Group XXXIV] In a lubrication system the tank containing the main body of oil in circulation is provided with two or more screens 17-19 for separating air…
A mould is made from burnt clay mixed with silicious material, sodium or potassium silicate or both, and a small quantity of acid or metal chloride or both. 20 to 70 parts of the clay may be mixed with 25 to 75 of sand, 2 to 10 of the silicate, which may be in the form of…
516,347. Alloys: annealing. HALL, H. C., and GRESHAM, H. E. June 3, 1938, No. 16665. [Classes 72 and 82 (i)] Copper alloys, particularly for sleeve valves and other parts of internal combustion engines, contain 6.5-9.2 per cent. of aluminium, 0.4-1 per cent. of chromium, 0.5-2…
Engineering parts are provided with coatings, resistant to stress and corrosion, formed of an alloy of the following composition:-Al 7.5-13.5 per cent, Cr 9.0-25.0 per cent, Mo 0.1-5.0 per cent, Co 0.1-1.0 per cent, Ni the balance. The alloy may include one or more of the…
600,067. Making engine sleeve-valves. GRESHAM, H. E., and HALL, B. Nov. 1, 1944, No. 21377. [Classes 83 (ii) and 83 (iv)] Altering molecular structure.-Finished or partly finished sleeve-valves of internal-combustion engines &c. are strain-hardened by application of a direct…
Nickel chromium alloys consisting of at least 50 per cent Ni (which may be replaced by Co up to 40 per cent of the alloy), 5-45 per cent Cr, and 40 per cent (max.) of the following addition elements, 1 per cent (max.) C, 5 per cent (max.) Ti or Si, 25 per cent (max.) Mo and 18…