A process for oxygen-initiated hydrobromination of propene to form a crude reaction mixture of 95 GC area % n-propyl bromide. The process includes feeding an oxygen-containing gas, propene and hydrogen bromide into a liquid phase mixture comprised of n-propyl bromide and…
Hall Tyson J
Processes are provided for recovering bromine values from brominated flame retardant materials in the form of HBr or Br2 and for using such recovered HBr and/or Br2 to reduce mercury emissions during coal combustion.
Processes for producing C2+ hydrocarbons are provided. Such processes use Br2, HBr, and/or heat that are produced by such processes, thus providing commercially efficient processes. The process can comprise (a) producing HBr and methyl bromide using a bromine source and a gas…
SO 3 is formed from a replenished circulating inventory of fresh and recycled SO 2 . Also, a feed stream of replenished SO 2 is heated by indirect heat exchange with a hot stream of SO 2 and SO 3 whereby the hot stream is cooled for separating the two gases. The heated feed…
Sulfur trioxide is formed by a process wherein a first gaseous stream comprised of S02, SO3, and oxygen and/or air is passed into a bed of a vanadium-containing catalyst that oxidizes S02 to S03and that releases therefrom a second gaseous stream comprised of sulfur trioxide.…
Processes are provided for conjointly producing Br 2 and a concentrated aqueous solution containing at least about 5 wt % CaCI 2 , based on the weight of the concentrated aqueous solution, from an HBr-rich recycle stream and a feed brine dilute in CaCI 2 . wherein the aqueous…
Processes are provided for conjointly producing Br 2 and a concentrated aqueous solution containing at least about 5 wt % CaCl 2 , based on the weight of the concentrated aqueous solution, from an HBr-rich recycle stream and a feed brine dilute in CaCl 2 . wherein the aqueous…
Processes are provided for conjointly producing Br 2 , a concentrated aqueous solution containing CaCI 2 , and Cl 2 from an aqueous HBr-rich stream and a feed brine dilute in CaCI 2 that comprises NaCI. Such processes can comprise feeding the aqueous HBr-rich stream and the feed…
SO 3 is formed from a replenished circulating inventory of fresh and recycled SO 2 . Also, a feed stream of replenished SO 2 is heated by indirect heat exchange with a hot stream of SO 2 and SO 3 whereby the hot stream is cooled for separating the two gases. The heated feed…
Processes are provided for conjointly producing Br2 and a concentrated aqueous solution containing at least about 5 wt% CaCI2, based on the weight of the concentrated aqueous solution, from an aqueous HBr rich stream and, optionally, a feed brine dilute in CaCI2. Such processes…
Processes are provided for conjointly producing Br2 and a concentrated aqueous solution containing at least about 5 wt% CaCI2, based on the weight of the concentrated aqueous solution, from an HBr-rich recycle stream and a feed brine dilute in CaCI2. wherein the aqueous HBr-rich…
Processes are provided for catalytic oxidation of bromide to bromine by use of oxygen at temperatures of at least about 315°C in the presence of a cerium-containing compound, such as a cerium bromide catalyst, wherein the produced stream comprising Br2 and H2O is directly cooled…
Processes are provided for conjointly producing Br2 and a concentrated aqueous solution containing at least about 5 wt % CaCI2, based on the weight of the concentrated aqueous solution, from an aqueous HBr rich stream and, optionally, a feed brine dilute in CaCI2. Such processes…
A process for oxygen-initiated hydrobromination of propene to form a crude reaction mixture of 95 GC area % n-propyl bromide. The process includes feeding an oxygen-containing gas, propene and hydrogen bromide into a liquid phase mixture comprised of n-propyl bromide and…
A process for oxygen-initiated hydrobromination of propene to form a crude reaction mixture of 95 GC area % n-propyl bromide. The process includes feeding an oxygen-containing gas, propene and hydrogen bromide into a liquid phase mixture comprised of n-propyl bromide and…
Methods are provided for regenerating catalyst compositions useful in processes for converting methane to useful hydrocarbons. The methods comprise applying voltage across the catalyst compositions.
Methods are provided for converting methane to useful hydrocarbons. In the methods provided, a fluid comprising methane and hydrogen is combined with a catalyst composition derived from at least an aluminum compound, such.as an aluminum halide, an aluminum alkyi, or a aluminum…
Methods are provided for converting methane to useful hydrocarbons. In the methods provided, a fluid comprising methane and hydrogen is combined with a catalyst composition derived from at least an aluminum compound, such.as an aluminum halide, an aluminum alkyi, or a aluminum…
Processes are provided for conjointly producing Br<SUB>2</SUB>, a concentrated aqueous solution containing CaCI<SUB>2</SUB>, and Cl<SUB>2</SUB> from an aqueous HBr-rich stream and a feed brine dilute in CaCI<SUB>2</SUB> that…
Processes are provided for conjointly producing Br2, a concentrated aqueous solution containing CaCI2, and Cl2 from an aqueous HBr-rich stream and a feed brine dilute in CaCI2 that comprises NaCI. Such processes can comprise feeding the aqueous HBr-rich stream and the feed brine…
Processes are provided for conjointly producing Br2 and a concentrated aqueous solution containing at least about 5 wt% CaCI2, based on the weight of the concentrated aqueous solution, from an aqueous HBr rich stream and, optionally, a feed brine dilute in CaCI2. Such processes…
Processes are provided for conjointly producing Br2 and a concentrated aqueous solution containing at least about 5 wt% CaCI2, based on the weight of the concentrated aqueous solution, from an HBr-rich recycle stream and a feed brine dilute in CaCI2. wherein the aqueous HBr-rich…
Processes for producing C2 + hydrocarbons are provided. Such processes use Br2, HBr, and/or heat that are produced by such processes, thus providing commercially efficient processes. The process can comprise (a) producing HBr and methyl bromide using a bromine source and a gas…
Processes are provided for recovering bromine values from brominated flame retardant materials in the form of HBr or Br2 and for using such recovered HBr and/or Br2 to reduce mercury emissions during coal combustion.
SO 3 is formed from a replenished circulating inventory of fresh and recycled SO 2 . Also, a feed stream of replenished SO 2 is heated by indirect heat exchange with a hot stream of SO 2 and SO 3 whereby the hot stream is cooled for separating the two gases. The heated feed…