A method of manufacturing a xerogel monolith having a pore diameter distribution includes preparing a first solution comprising metal alkoxide and preparing a second solution comprising a catalyst. A third solution is prepared by mixing the first solution and the second solution…
Assignee / Organization
Halefoglu Yasar
4Total Forward Citations
1Indexed Patents
4Avg Citations / Patent
1Portfolio H-Index