A racemic complex of formula (I), wherein ∙ M is zirconium or hafnium; ∙ each X is a sigma ligand; ∙ L is a divalent bridge selected from -R' 2 C-, -R' 2 C-CR' 2 , -R' 2 Si-, - R' 2 Si-SiR' 2 -, -R' 2 Ge-, wherein each R' is independently a…
Hafner Norbert
A polypropylene homopolymer with a melting point of less than 147°C, a percentage of 2,1 errors of at least 1% and a xylene soluble fraction of less than 0.5 wt%.
A heterophasic polypropylene resin comprising a polypropylene homopolymer matrix phase (A) and an ethylene-propylene copolymer phase (B) dispersed within the matrix, wherein the xylene soluble fraction of the heterophasic polypropylene resin is in the range 20 to less than 50…
A heterophasic polypropylene resin comprising a polypropylene homopolymer matrix phase (A) and an ethylene-propylene copolymer phase (B) dispersed within the matrix, wherein the xylene soluble fraction of the heterophasic polypropylene resin is in the range 20 to less than 50 wt…
The present invention relates to a process for preparing a propylene random copolymer comprising polymerisation of propylene with a comonomer, said comonomer being ethylene or an α-olefin comprising at least four carbon atoms, in the presence of a catalyst in a multistage…
Propylene copolymer (a) comprising at least 1-butene as a comonomer, (b) having a comonomer content in the range of 1.0 to 3.0 wt.-%, (c) having a xylene soluble fraction equal or below 2.5 wt.-%, and (d)being partially crystallized in the ß-modification.
A racemic complex of formula (I), wherein M is zirconium or hafnium; each X is a sigma ligand; L is a divalent bridge selected from —R′ 2 C—, —R′ 2 C—CR′ 2 , —R′ 2 Si—, —R′ 2 Si—SiR′ 2 —, —R′ 2 Ge—, wherein each R′ is independently a hydrogen atom, C 1-20 -hydrocarbyl, tri(C…
A luminous device includes at least one radiation-emitting semiconductor chip including at least two emission regions arranged spaced apart in a lateral direction, wherein each emission region includes at least one active zone that emits electromagnetic radiation; and a drive…
Propylene copolymer (a) comprising at least 1-butene as a comonomer, (b) having a comonomer content in the range of 1.0 to 3.0 wt.-%, (c) having a xylene soluble fraction equal or below 2.5 wt.-%, and (d) being partially crystallized in the β-modification.
Propylene copolymer a. comprising at least 1-hexene as a comonomer, b. having a comonomer content in the range of 1.0 to 3.0 wt.-%, c. having a xylene soluble fraction equal or below 2.5 wt.-%, and d. being partially crystallized in the β-modification.
The present invention relates to a process for preparing a propylene random copolymer comprising polymerisation of propylene with a comonomer, said comonomer being ethylene or an α-olefin comprising at least four carbon atoms, in the presence of a catalyst in a multistage…
Propylene copolymer a. comprising at least 1-hexene as a comonomer, b. having a comonomer content in the range of 1.0 to 3.0 wt.-%, c. having a xylene soluble fraction equal or below 2.5 wt.-%, d. having a polydispersity index (PI) of equal or below 4.0 Pa −1 , and e. being…
A polypropylene homopolymer with a melting point of less than 147° C., a percentage of 2.1 errors of at least 1% and a xylene soluble fraction of less than 0.5 wt %.
Propylene copolymer a. comprising at least 1-hexene as a comonomer, b. having a comonomer content in the range of 1.0 to 3.0 wt.-%, c. having a xylene soluble fraction equal or below 2.5 wt.-%, d. having a polydispersity index (PI) of equal or below 4.0 Pa-1, and e. being…
The present invention relates to a process for preparing a propylene random copolymer comprising polymerisation of propylene with a comonomer, said comonomer being ethylene or an α-olefin comprising at least four carbon atoms, in the presence of a catalyst in a multistage…
A heterophasic polypropylene resin comprising a polypropylene homopolymer matrix phase (A) and an ethylene-propylene copolymer phase (B) dispersed within the matrix, wherein the xylene soluble fraction of the heterophasic polypropylene resin is in the range 20 to less than 50 wt…
A polypropylene homopolymer with a melting point of less than 147° C., a percentage of 2.1 errors of at least 1% and a xylene soluble fraction of less than 0.5 wt %.
Propylene copolymer (a) comprising at least 1-butene as a comonomer, (b) having a comonomer content in the range of 1.0 to 3.0 wt.-%, (c) having a xylene soluble fraction equal or below 2.5 wt.-%, and (d) being partially crystallized in the β-modification.
A racemic complex of formula (I), wherein M is zirconium or hafnium; each X is a sigma ligand; L is a divalent bridge selected from —R′ 2 C—, —R′ 2 C—CR′ 2 , —R′ 2 Si—, —R′ 2 Si—SiR′ 2 —, —R′ 2 Ge—, wherein each R′ is independently a hydrogen atom, C 1-20 -hydrocarbyl, tri(C…
A polypropylene homopolymer with a melting point of less than 147°C, a percentage of 2,1 errors of at least 1% and a xylene soluble fraction of less than 0.5 wt%.
Propylene copolymer a. comprising at least 1-hexene as a comonomer, b. having a comonomer content in the range of 1.0 to 3.0 wt.-%, c. having a xylene soluble fraction equal or below 2.5 wt.-%, and d. being partially crystallized in the β-modification.