A fusion-cast refractory is provided. The refractory comprises 0.8% to 2.5% Al 2 O 3 , 4.0% to 10.0% SiO 2 86% to 95% ZrO 2 , 0.1% to 1.2% B 2 O 3 , up to 0.04% Na 2 O, up to 0.4% CaO, up to 0.1% Fe 2 O 3 and up to 0.25% TiO 2 ..
Assignee / Organization
Gupta Amul
45Total Forward Citations
2Indexed Patents
22Avg Citations / Patent
2Portfolio H-Index
A method includes containing a high-temperature alkali salt containing environment using a refractory containment liner containing MgAl 2 O 4 spinel. A method, includes forming a refractory brick containing MgAl 2 O 4 spinel having an exterior chill zone defined by substantially…