Patents
US 2012165242 A1#6439234 Most Cited · 15 citations1.1/yr · PR 2.20PendingUS · Application
Polymers for high-surfactant formulations

A detergent composition having at least two components. The first component is from 14 to 50 wt % surfactants. The second component is from 0.05 to 4 wt % of a polymer which has polymerized residues of 40 to 65 wt % C 1 -C 18 alkyl (meth)acrylates and 25 to 55 wt % C 3 -C 6…

US 2011046023 A1#16805681 Most Cited · 6 citations0.4/yr · PR 2.07PendingUS · Application
Scale and corrosion inhibitors for high temperature and pressure conditions

The present invention relates to a method for inhibiting scale and corrosion in aqueous systems, for example, under high temperature and pressure conditions such as temperatures up to 250° C. and/or pressures up to 10000 psi (i.e., about 68.9 MPa). The method involves providing…

US 2011237745 A1#24866900 Most Cited · 4 citations0.3/yr · PR 1.37PendingUS · Application
Method for producing hydrophobically modified acrylic rheology modifers

A method for preparing hydrophobically modified rheology modifiers; said method comprising polymerizing a monomer mixture having two or more components. The first component is H 2 C═C(R)C(O)X(CH 2 CH 2 O) n (CH(R′)CH 2 O) m R″ or H 2 C═C(R)C 6 H 4 C(CH 3 ) 2 NHCO 2 (CH 2 CH 2 O)…

US 8,158,561 B2#37023503 Most Cited · 2 citations0.1/yr · PR 1.13ActiveUS · Utility
Scale and corrosion inhibitors for high temperature and pressure conditions
Inventors: Greyson Eric, Manna Joseph, Mehta Somil ChandrakantAssignee: Greyson Eric, Manna JosephFiled 2010-08-13 · Granted 2012-04-17

The present invention relates to a method for inhibiting scale and corrosion in aqueous systems, for example, under high temperature and pressure conditions such as temperatures up to 250° C. and/or pressures up to 10000 psi (i.e., about 68.9 MPa). The method involves providing…