Green Robert A
Conjugate fibers are prepared in which at least one segment is a mixture of a high-D PLA resin and a high-L PLA resin. These segments have crystallites having a crystalline melting temperature of at least 200° C. At least one other segment is a high-D PLA resin or a high-L PLA…
Polylactide fibers are made from a blend of polylactides. One of the polylactides has a ratio of R-lactic and S-lactic units from 8:92 to 92:8. The second polylactide has a ratio of the R-lactic and S-lactic units of >97:3 or <3:97. The ratio of the R-lactic units to…
PLA stereocomplex fibers are made by separately melting a high-D PLA starting resin and a high-L starting resin, mixing the melts and spinning the molten mixture. Subsequent heat treatment introduces high-melting “stereocomplex” crystallinity into the fibers. The process can…
Conjugate fibers are prepared in which at least one segment is a mixture of a high-D PLA resin and a high-L PLA resin. These segments have crystallites having a crystalline melting temperature of at least 200° C. At least one other segment is a high-D PLA resin or a high-L PLA…
PLA stereocomplex fibers are made by separately melting a high-D PLA starting resin and a high-L starting resin, mixing the melts and spinning the molten mixture. Subsequent heat treatment introduces high-melting “stereocomplex” crystallinity into the fibers. The process can…
Polylactide fibers are made from a blend of polylactides. One of the polylactides has a ratio of R-lactic and S-lactic units from 8:92 to 92:8. The second polylactide has a ratio of the R-lactic and S-lactic units of >97:3 or <3:97. The ratio of the R-lactic units to…