A process for producing an epoxidized elastomeric polymer by feeding at least one elastomeric polymer containing ethylenic unsaturation to a mixing device; feeding at least one hydrogen peroxide precursor to the mixing device; feeding at least one carboxylic acid or a derivative…
Grassi Lisa
Tire comprising: - a carcass structure of a substantially toroidal shape, having opposite lateral edges associated with respective right-hand and left-hand bead structures, said bead structures comprising at least one bead core and at least one bead filler; - a belt structure…
Tire comprising at least one structural element including a crosslinked elastomeric material obtained by crosslinking a crosslinkable elastomeric composition comprising a crosslinkable elastomeric base comprising at least 30 phr, preferably of from 50 phr to 100 phr, of at least…
Tire for a motorcycle said tire having a transverse curvature ratio (f/C) of at least 0.20 and a total height/width (H/C) ratio of at least 0.5, a radial carcass (2) comprising textile cords made from lyocell fibre.
Optical fiber comprising: a) a glass portion; b) at least one protective coating layer disposed to surround said glass portion; said protective coating layer having a modulus of elasticity value between -40 °C and +60 °C comprised between 5 MPa and 600 MPa, preferably not higher…
Tyre comprising at least one structural element obtained by crosslinking a crosslinkable elastomeric compositon comprising: (a) a crosslinkable elastomeric base comprising at least 10 phr, preferably from 30 phr to 100 phr, of (al) at least one epoxidized elastomeric polymer…
An optical fiber having: a) a glass portion; and b) at least one protective coating layer disposed to surround the glass portion, the protective coating layer having a modulus of elasticity value between −40° C. and +60° C. between 5 MPa and 600 MPa, preferably not higher than…
Process for producing an epoxidized elastomeric polymer comprising: feeding at least one elastomeric polymer containing ethylenic unsaturations to a mixing device; feeding at least one hydrogen peroxide precursor to said mixing device; feeding at least one carboxylic acid or a…
Method for producing a crosslinkable elastomeric composition comprising: (a) at least one first elastomeric polymer; (b) at least one layered material having an individual layer thickness of from 0.01 nm to 30 nm, preferably of from 0.05 nm to 15 nm; (c) at least one vulcanizing…
A tire for a motorcycle having a transverse curvature ratio of at least 0.20 and a total height/width ratio of at least 0.5, includes a radial carcass including textile cords made from lyocell cellulose fibre.
Method for producing a crosslinkable elastomeric composition including: (a) at least one first elastomeric polymer; (b) at least one layered material having an individual layer thickness of 0.01 nm to 30 nm, preferably of 0.05 nm to 15 nm; and (c) at least one vulcanizing agent;…
A process for producing a composite material includes the following steps: (a) melting at least one polyester having an inherent viscosity higher than or equal to 0.5 dl/g, preferably 0.6 dl/g to 1.2 dg/l; (b) cooling said polyester so as to obtain a polyester having a…
Process for producing a composite material comprising the following steps: (a) melting at least one polyester having an inherent viscosity (I.V.) higher than or equal to 0.5 dl/g, preferably of from 0.6 dl/g to 1.2 dg/l; (b) cooling said polyester so as to obtain a polyester…