The low shear, slurry viscosity of a kaolinitic clay that is contaminated with one or more forms of expanding clay is reduced by mixing the clay with a source of cationic potassium and then heating the potassium-treated clay to a temperature of at least about 100° C.
Ginn Michael W
A method of recovering a mineral product from carpet by preparing a feed of carpet pieces; thermally separating organic components from mineral components in the carpet by heating the carpet pieces to a particle bed temperature in the range of 600° C. to 1000° C., wherein the…
High brightness, whiteness and opacity calcium carbonate pigments (44 and 58) may be produced by magnetic separation (34 and 50). A composition of matter comprising high brightness calcium carbonate pigments (44 and 58) produced by using magnetic separation (34 and 50) on a…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
A method of recovering a mineral product from carpet by preparing a feed of carpet pieces; thermally separating organic components from mineral components in the carpet by heating the carpet pieces to a particle bed temperature in the range of 600° C. to 1000° C., wherein the…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
High brightness, whiteness and opacity calcium carbonate pigments (44 and 58) may be produced by magnetic separation (34 and 50). A composition of matter comprising high brightness calcium carbonate pigments (44 and 58) produced by using magnetic separation (34 and 50) on a…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
A thermally processed clay product as well as blends of the product with other fillers is produced at or in proximity to the end-use site to provide a product having improved properties. The Pyroflex Pigment Recovery System in which thermal engineering is employed in the…
High brightness, whiteness and opacity calcium carbonate pigments (44 and 58) may be produced by magnetic separation (34 and 50). A composition of matter comprising high brightness calcium carbonate pigments (44 and 58) produced by using magnetic separation (34 and 50) on a…