Industrial materials can be efficiently pan granulated by grinding the material to 95% minus 150 mesh, feeding this to a pan in conjunction with 1 to 15% seed materials and applying binder solution such that the free moisture content of the green ball is between 8-13% by weight…
Assignee / Organization
Gary Derdall
0Total Forward Citations
1Indexed Patents
0Avg Citations / Patent
0Portfolio H-Index
Key Inventors: Derdall Gary Ma Siu L