A method of brazing brass parts without oxidation of zinc, which is contained in the parts, during brazing of the parts with phosphorous bronze solder at relatively low temperature of 630-700° C., the brazing being made by making the wall of brazing furnace or muffle of carbon…
Fuse Masashi
When an aluminum product is preheated to about 500ºC in preheating furnace (6) before flux brazing of the aluminum product in a heating furnace, the heating time for brazing the aluminum product through heating the same in a continuous-atmosphere furnace including preheating…
The object of this invention is to have shorter sealing chambers (preheating chamber and gradual cooling chamber) located before and after the brazing atmospheric chamber, to make higher sealing of the atmosphere, and to prevent the scratch caused by the conventional curtains…
[PROBLEMS] To provide a magnetic field detecting apparatus and an electronic compass using the same wherein the strength of an external magnetic field can be determined even under an environment having relatively large external disturbance. [MEANS FOR SOLVING PROBLEMS] A current…
When the input flux density B is within ±S1, the difference in output voltage between an MR sensor (11) and an MR sensor (12) is substantially 0. When the input flux density B is between S1 and S2, the differential voltage between the output voltage V1 from the MR sensor (11)…